In order to explore the application of click chemistry in the field of elastomer materials, the comparison between the properties of polyurethane and polytriazole elastomers has been carried out. Propargyl-terminated ethylene oxide-tetrahydrofuran copolymer (PTPET) has been prepared from the ethylene oxide-tetrahydrofuran copolymer (PET) by end modification. Using polyisocyanate N100 and polyazide compounds as cross-linkers, PET polyurethane and PTPET polytriazole elastomers have been prepared through urethane and copper-catalyzed azide-alkyne huisgen [3+2] dipolar cycloaddition reactions, respectively. Mechanical properties indicate that, to be different from those of polyurethane elastomers, the modulus E and stress σb of polytriazole elastomers increase at first, and then decrease with the increase in R. At around the stoichiometric ratio, the modulus E and stress σb reach a maximum, and the strain εb reaches a minimum. Swelling tests demonstrate that the Mc of polytriazole elastomers has a minimum value at the stoichiometric ratio. The dynamic mechanical analysis indicates that both polyurethane and polytriazole elastomers have the same glass transition temperature of -64°C, although polytriazole elastomers exhibit lower dissipation factor tan δ. Thermal analysis shows that polytriazole elastomers have better thermal stability than polyurethane elastomers.

Original languageEnglish
Pages (from-to)314-321
Number of pages8
JournalPolymers for Advanced Technologies
Volume25
Issue number3
DOIs
Publication statusPublished - Mar 2014

Keywords

  • Click chemistry
  • Elastomers
  • PTPET
  • Polytriazole
  • Polyurethane

Fingerprint

Dive into the research topics of 'Comparison between properties of polyether polytriazole elastomers and polyether polyurethane elastomers'. Together they form a unique fingerprint.

Cite this