Solid-state alkaline metal batteries are highly sought out for their improved energy density and security over the current lithium-ion batteries. However, their practical application is heavily hindered by the interfacial issues originating from the solid electrolyte/electrode mismatch. This work demonstrates that a CuO coating layer as an active interphase can thoroughly promote the intimate contact between a Na3Zr2Si2PO12 solid electrolyte and a Na metal anode through an in situ conversion reaction. The resultant Cu/Na2O matrix forms a mixed electron/ion conducting scaffold, which facilitates stable and homogeneous Na metal plating without dendrite formation. Moreover, the symmetric Na metal cell realizes impressively steady plating/stripping cycles for 5000 h even under a high current density of 0.3 mA cm−2. The novelty is further manifested as a room-temperature solid-state Na metal full battery of Na3V1.5Al0.5(PO4)3|CuO@NZSPO|Na is assembled and exhibits a highly reversible cyclability (99.85% coulombic efficiency and 99.0% capacity retention) under a charge/discharge rate of 5 C for 2250 cycles. This work effectively solves the interfacial issues at the Na metal/solid electrolyte interface and provides a convenient way toward high-performance solid-state Na metal batteries operated at room temperature.

源语言英语
文章编号2204487
期刊Small
18
45
DOI
出版状态已出版 - 10 11月 2022

指纹

探究 'Uniform Na Metal Plating/Stripping Design for Highly Reversible Solid-State Na Metal Batteries at Room Temperature' 的科研主题。它们共同构成独一无二的指纹。

引用此

Miao, R., Wang, C., Li, D., Sun, C., Li, J., & Jin, H. (2022). Uniform Na Metal Plating/Stripping Design for Highly Reversible Solid-State Na Metal Batteries at Room Temperature. Small, 18(45), 文章 2204487. https://doi.org/10.1002/smll.202204487