Study on weld defect testing technology based on the method of magnetic memory

Hong Guang Liu*, Wei Min Zhang, Zhao Xia Wang, Jun Jie Yuan

*此作品的通讯作者

科研成果: 期刊稿件文章同行评审

8 引用 (Scopus)

摘要

To study on the changes of magnetic memory signals of defects in the weld seam, a magnetic dipole model of weld seam in earth magnetic field was established. The change curves with defect and without defect in the weld seam were simulated. According to the changes of curves, the law of magnetic field changes when there were defects in the weld seam was obtained. The magnetic memory signals of the self made weld samples were tested to compare with the model. The testing curves with defects in the weld seam and the simulated curves matched each other well. The magnetic dipole model established can reflect the real situation of magnetic memory signals in the weld seam, and can be used to estimate the defects in the weld seam.

源语言英语
页(从-至)811-814
页数4
期刊Beijing Ligong Daxue Xuebao/Transaction of Beijing Institute of Technology
27
9
出版状态已出版 - 9月 2007

指纹

探究 'Study on weld defect testing technology based on the method of magnetic memory' 的科研主题。它们共同构成独一无二的指纹。

引用此