TY - JOUR
T1 - Preparation of integrated carbon fiber stitched fabric reinforced (SiBCN) ceramic/resin double-layered composites for ablation resistance, thermal insulation and compression resistance performance
AU - Xia, Chunlei
AU - Xie, Weihua
AU - Meng, Songhe
AU - Gao, Bo
AU - Ye, Jinrui
N1 - Publisher Copyright:
© 2024 Elsevier Ltd
PY - 2024/6/16
Y1 - 2024/6/16
N2 - This paper reports a novel integrated carbon fiber fabric reinforced ceramic/resin double-layered composite. The composites were prepared by a low energy consumption process of stratified impregnate pyrolysis. The double-layered composites consist of an amorphous SiBCN ceramic upper layer and a SiBCN resin bottom layer. In the ablation experiment, the temperature of the composite material's ablated surface exceeded 1850 °C, while the temperature of the backside remained below 70 °C within 60 s of ablation. Even after 90 s of ablation, the backside temperature was still significantly lower than the theoretical application temperature of SiBCN resin. The ablated surface has no visible pits or cracks. The maximum mass ablation rate and line ablation rate were −0.01259 mg/s and 0.000933 mm/s, respectively. High-density amorphous SiBCN ceramic layer effectively play the role of high temperature and ablation resistance. In addition, the compressive strengths of the composites before and after ablation were above 340 MPa. Integrated composites that combine anti-ablation, insulation, and compression resistance have potential in aerospace applications.
AB - This paper reports a novel integrated carbon fiber fabric reinforced ceramic/resin double-layered composite. The composites were prepared by a low energy consumption process of stratified impregnate pyrolysis. The double-layered composites consist of an amorphous SiBCN ceramic upper layer and a SiBCN resin bottom layer. In the ablation experiment, the temperature of the composite material's ablated surface exceeded 1850 °C, while the temperature of the backside remained below 70 °C within 60 s of ablation. Even after 90 s of ablation, the backside temperature was still significantly lower than the theoretical application temperature of SiBCN resin. The ablated surface has no visible pits or cracks. The maximum mass ablation rate and line ablation rate were −0.01259 mg/s and 0.000933 mm/s, respectively. High-density amorphous SiBCN ceramic layer effectively play the role of high temperature and ablation resistance. In addition, the compressive strengths of the composites before and after ablation were above 340 MPa. Integrated composites that combine anti-ablation, insulation, and compression resistance have potential in aerospace applications.
KW - Heat treatment
KW - High-temperature properties
KW - Hybrid composites
KW - Multifunctional properties
KW - SEM
UR - http://www.scopus.com/inward/record.url?scp=85191728686&partnerID=8YFLogxK
U2 - 10.1016/j.compscitech.2024.110629
DO - 10.1016/j.compscitech.2024.110629
M3 - Article
AN - SCOPUS:85191728686
SN - 0266-3538
VL - 252
JO - Composites Science and Technology
JF - Composites Science and Technology
M1 - 110629
ER -