Low-temperature densification of TiB2 ceramic by the spark plasma sintering process with Ti as a sintering aid

Zhao Hui Zhang*, Xiang Bo Shen, Fu Chi Wang, Shu Kui Lee, Qun Bo Fan, Mao Sheng Cao

*此作品的通讯作者

科研成果: 期刊稿件文章同行评审

75 引用 (Scopus)

摘要

The microstructure and the mechanical properties of TiB2 ceramics synthesized by the spark plasma sintering (SPS) process with Ti sinter-aid were investigated. The results indicate that the addition of 2.5 wt.% Ti significantly decreases the densification temperature of the TiB2 ceramic. The TiB2 ceramic sintered at 1650 °C exhibits the highest relative density of 99.1%, a microhardness of 26.8 ± 1.6 GPa, a flexural strength of 558 ± 39 MPa and a fracture toughness of 5.9 ± 0.3 MPa m1/2.

源语言英语
页(从-至)167-170
页数4
期刊Scripta Materialia
66
3-4
DOI
出版状态已出版 - 2月 2012