The laser powder bed fusion (PBF-LB) process provides great potential for additive manufacturing of Invar 36 alloy, which possesses a unique low coefficient of thermal expansion. However, the high-temperature tensile behavior of PBF-LB processed Invar 36 alloy has not been explored, severely restricting its applications. Hence, herein, in-situ X-ray computed tomography (XCT) tensile tests were conducted at 200 °C and 600 °C for PBF-LB processed Invar 36 alloy, and the microstructure after heat treatment, fracture morphology, post-mortem microstructure, and nano-precipitates were observed. The in-situ XCT analysis of damage evolution reveals that the tensile behavior at elevated temperatures is sensitive to numerous closely spaced lack-of-fusion (LOF) pores with relatively large equivalent diameters, distributed in the adjacent melt pools or deposited layers. These LOF pores promote the stress concentration and facilitate rapid crack propagation, resulting in a significantly diminished strength and ductility. In contrast, the small number of metallurgical and keyhole pores, possessing large spacing and relatively high sphericity, have negligible influence on the tensile behavior. Therefore, Invar 36 alloy with only metallurgical and keyhole pores can be considered defect-free, displaying an excellent yield strength of 360.0 MPa and a considerable elongation of 65.0% at 200 °C. However, as the temperature increases to 600 °C, both the yield strength and elongation show a marked decrease to 150.0 MPa and 5.4%, respectively. This weakening is accompanied by the observation of a brittle fracture and the formation of secondary cracks. The degradation in mechanical properties can be attributed to the decomposition of Cr-containing SiP2O7, which leads to the formation of numerous small-sized SiO2 and P2O5 precipitates at 600 °C. These precipitates induce embrittlement of the grain boundaries and contribute to the formation of secondary cracks. The anomalous brittle fracture observed is attributed to the intergranular fracture mode, which results from the low grain boundary energy as well as the decomposition of nanoprecipitates. Additionally, the perpendicular orientation of flatter columnar grain boundaries to the loading direction plays a role in the formation of secondary cracks. This high-temperature mechanical performance of strength, elongation, failure mode, and corresponding microcosmic mechanism advances the understanding and widespread application of PBF-LB processed Invar 36 alloy.

源语言英语
文章编号104072
期刊Additive Manufacturing
83
DOI
出版状态已出版 - 5 3月 2024

指纹

探究 'In-situ X-ray computed tomography of high-temperature tensile behavior for laser powder bed fused Invar 36 alloy' 的科研主题。它们共同构成独一无二的指纹。

引用此