The phase transitions of ε-CL-20 coated with desensitizers [paraffin wax (PW), microcrystal wax (MW), graphite, molybdenum disulfide, tungsten disulfide, and graphite fluoride] were investigated using powder X-ray diffraction (PXRD) and differential scanning calorimetry (DSC). The thermal behavior of ε-CL-20 and ε-CL-20 coated with desensitizers was analyzed, and the compatibility of ε-CL-20 with the desensitizers was assessed using vacuum stability tests. The characteristics of several desensitizers were measured, and their effects on the friction and impact sensitivity of coarse and fine ε-CL-20 crystals were analyzed. The results indicate that graphite decreased the critical temperature of phase transition. The phase transition of DSC results is consistent with the PXRD data. ε-CL-20 was compatible with all the desensitizers studied. Molybdenum disulfide markedly lowered the impact sensitivity; PW and MW lowered the friction sensitivity of ε-CL-20. The molybdenum disulfide/PW compound system reduced both the friction and impact sensitivity of ε-CL-20.
源语言 | 英语 |
---|---|
页(从-至) | 111-120 |
页数 | 10 |
期刊 | Journal of Energetic Materials |
卷 | 36 |
期 | 1 |
DOI | |
出版状态 | 已出版 - 2 1月 2018 |