2024Al and SiC/2024Al were used to encapsulate the AD95 Al 2O3 ceramics by Vacuum-high Pressure Infiltration Method. Their anti-bullet properties are not excellent with Efm of 5.17 and 4.65 respectively, and is far lower than Efm of the ceramic without encapsulation. The latter one can generate higher hydrostatic pressure between the bullet and ceramic during penetration process. However, in encapsulated targets, the ductile materials in front of the ceramic can decelerate the bullet, so the pressure between bullet and ceramic is not great enough to break the bullet. Propagated microcracks along with the bonding interface were observed in plates consisting of encapsulated Al2O3. These microcraks lead to the interfacial debonding between Al2O3 and encapsulating materials. Consequently, the anti-bullet property of the ceramic encapsulated by metal or composite is depressed. Further more, the different interface bonding conditions and fracture modes cause the discrepancy of anti-bullet property in two kinds of targets with encapsulation structure.

源语言英语
主期刊名High-Performance Ceramics VII
出版商Trans Tech Publications Ltd.
494-499
页数6
ISBN(印刷版)9783037854259
DOI
出版状态已出版 - 2012
活动7th China International Conference on High-Performance Ceramics, CICC-7 - Xiamen, 中国
期限: 4 11月 20117 11月 2011

出版系列

姓名Key Engineering Materials
512-515
ISSN(印刷版)1013-9826
ISSN(电子版)1662-9795

会议

会议7th China International Conference on High-Performance Ceramics, CICC-7
国家/地区中国
Xiamen
时期4/11/117/11/11

指纹

探究 'Anti-bullet property of encapsulated AD95 Al2O3 ceramic' 的科研主题。它们共同构成独一无二的指纹。

引用此