In this study, indium oxide (In2O3) thin-film transistors (TFTs) are fabricated by two kinds of low temperature solution-processed technologies (Ta ≤ 300 °C), i.e., water-based (DIW-based) process and alkoxide-based (2-ME-based) process. The thickness values, crystallization properties, chemical structures, surface roughness values, and optical properties of In2O3 thin-films and the electrical characteristics of In2O3 TFTs are studied at different annealing temperatures. Thermal annealing at higher temperature leads to an increase in the saturation mobility (μsat) and a negative shift in the threshold voltage (VTH). The DIW-based processed In2O3-TFT annealed at 300 °C exhibits excellent device performance, and one annealed at 200 °C exhibits an acceptable μsat of 0.86 cm2/Vs comparable to that of a-Si:H TFTs, whereas the 2-ME-based TFT annealed at 300 °C exhibits an abundant μsat of 1.65 cm2/Vs and one annealed at 200 °C is inactive. The results are attributed to the fact that the DIW-based process induces a higher degree of oxidation and less defect states than the 2-ME-based process at the same temperature. The DIW-based process for fabricating the In2O3 TFT opens the way for the development of nontoxic, low-cost, and low-temperature oxide electronics.
Original language | English |
---|---|
Article number | 048504 |
Journal | Chinese Physics B |
Volume | 27 |
Issue number | 4 |
DOIs | |
Publication status | Published - Apr 2018 |
Keywords
- alkoxide-based process
- annealing temperature
- thin-film transistors
- water-based process