N2 - There are a number of attempts to release and recover the valuable metals from spent refinery catalysts by bioleaching, and the heat pretreatment is widely used to remove the oil-like compounds for better bioleaching performance. However, the irrational selection of high calcinations temperature of 600–800 °C not only resulted in high energy consumption but also might be cause lower bioleaching efficiencies of metals. In this work, Plackett-Burman design was used to optimize the heat treatment process and recognize the significant control factor. Especially, the mechanisms why low calcinations temperature of 400 °C had the best enhancement on the bioleaching performance of spent catalyst were expounded via microcosmic phase change analysis, biochemical leaching process analysis and bioleaching kinetics analysis. The results showed that the calcinations temperature greatly affected the bioleaching performance and the calcinations of 400 °C witnessed the maximum release efficiencies of 94% for Co and 100% for Mo, respectively; whereas poor bioleaching occurred with 200 or 600 °C. Further studies demonstrated the 400 °C-treatment removed the toxic oil-like compounds, excited the growth of cells, transformed refractory Co/Mo sulfides into tractable Co3O4/MoO3, reduced the percent of residual from, enabled more exposure of Co/Mo oxides at catalyst surface, which caused the best bioleaching performance.
AB - There are a number of attempts to release and recover the valuable metals from spent refinery catalysts by bioleaching, and the heat pretreatment is widely used to remove the oil-like compounds for better bioleaching performance. However, the irrational selection of high calcinations temperature of 600–800 °C not only resulted in high energy consumption but also might be cause lower bioleaching efficiencies of metals. In this work, Plackett-Burman design was used to optimize the heat treatment process and recognize the significant control factor. Especially, the mechanisms why low calcinations temperature of 400 °C had the best enhancement on the bioleaching performance of spent catalyst were expounded via microcosmic phase change analysis, biochemical leaching process analysis and bioleaching kinetics analysis. The results showed that the calcinations temperature greatly affected the bioleaching performance and the calcinations of 400 °C witnessed the maximum release efficiencies of 94% for Co and 100% for Mo, respectively; whereas poor bioleaching occurred with 200 or 600 °C. Further studies demonstrated the 400 °C-treatment removed the toxic oil-like compounds, excited the growth of cells, transformed refractory Co/Mo sulfides into tractable Co3O4/MoO3, reduced the percent of residual from, enabled more exposure of Co/Mo oxides at catalyst surface, which caused the best bioleaching performance.
KW - Bioleaching
KW - Enhancement effect
KW - Recovery of valuable metals
KW - Simultaneous release
KW - Spent refinery catalyst
KW - Thermal pre-treatment
UR - http://www.scopus.com/inward/record.url?scp=85094189112&partnerID=8YFLogxK
U2 - 10.1016/j.hydromet.2020.105389
DO - 10.1016/j.hydromet.2020.105389
M3 - Article
AN - SCOPUS:85094189112
SN - 0304-386X
VL - 198
JO - Hydrometallurgy
JF - Hydrometallurgy
M1 - 105389
ER -