Four La-Fe oxide samples with La/Fe atomic ratio y = 1.02 ∼ 0.68 (denoted as LayFe) were prepared by the citrate method. The samples had a decreased specific surface area with the La/Fe atomic ratio decreasing. XRD pattern proved that the sample La 0.94 Fe is single phase perovskite La 0.94 FeO 3-d . Phase composition of the samples was estimated by the Rietveld refinement method. XPS analyses indicate that La 3+ ions are enriched on surface of crystallites for all the samples, and surface carbonate ions are relatively abundant on the samples La 1.02 Fe and La 0.94 Fe. Catalytic activity for methane oxidation per unit surface area of the samples is in the order of La 0.68 Fe > La 0.76 Fe > La 0.94 Fe > La 1.02 Fe both in the presence and in the absence of gaseous oxygen. A reason for this order would be the higher concentration of Fe 3+ ion on the surface of the samples La 0.68 Fe and La 0.76 Fe.
源语言 | 英语 |
---|---|
页(从-至) | 709-714 |
页数 | 6 |
期刊 | Applied Surface Science |
卷 | 351 |
DOI | |
出版状态 | 已出版 - 1 10月 2015 |