N2 - Decreasing Y2O3-doped barium zirconate (BZY) sintering temperature is crucial for its implementation in solid oxide fuel cells (SOFC). Bismuth oxide as sintering aid for BZY is evaluated. It is found that 3 mol% Bi2O3 doped BZY (BZY-3) improves its shrinkage from 10.4% to 19.02% at about 1480 °C, with the maximum shrinkage rate increasing from -0.20 mm min-1 to -0.34 mm min-1. The activation energy for densification is 5.40 eV for BZY-3. The SEM images confirms that it is porous for BZY without Bi2O3 (BZY-0), but that less small pores could be seen for BZY-3 and 5 mol% Bi 2O3 doped BZY (BZY-5) sintered at 1400 °C for 24 h. Bi2O3 addition decreases the grain boundary conductivity for BZY-3 and BZY-5 obviously, but is less significant for BZY-2. It is 1.13 × 10-3 S cm-1 for BZY-2 in wet hydrogen atmosphere at 600 °C sintered at 1400 °C for 24 h, nearly equal to that of BZY-0. The open circuit voltage is 0.95 V, with the ionic transport number of 0.83 for BZY-2 under SOFC operating conditions.
AB - Decreasing Y2O3-doped barium zirconate (BZY) sintering temperature is crucial for its implementation in solid oxide fuel cells (SOFC). Bismuth oxide as sintering aid for BZY is evaluated. It is found that 3 mol% Bi2O3 doped BZY (BZY-3) improves its shrinkage from 10.4% to 19.02% at about 1480 °C, with the maximum shrinkage rate increasing from -0.20 mm min-1 to -0.34 mm min-1. The activation energy for densification is 5.40 eV for BZY-3. The SEM images confirms that it is porous for BZY without Bi2O3 (BZY-0), but that less small pores could be seen for BZY-3 and 5 mol% Bi 2O3 doped BZY (BZY-5) sintered at 1400 °C for 24 h. Bi2O3 addition decreases the grain boundary conductivity for BZY-3 and BZY-5 obviously, but is less significant for BZY-2. It is 1.13 × 10-3 S cm-1 for BZY-2 in wet hydrogen atmosphere at 600 °C sintered at 1400 °C for 24 h, nearly equal to that of BZY-0. The open circuit voltage is 0.95 V, with the ionic transport number of 0.83 for BZY-2 under SOFC operating conditions.
KW - Bismuth oxide
KW - Sintering aids
KW - Solid oxide fuel cells
KW - Yttria-doped barium zirconate
UR - http://www.scopus.com/inward/record.url?scp=84873333968&partnerID=8YFLogxK
U2 - 10.1016/j.jpowsour.2013.01.065
DO - 10.1016/j.jpowsour.2013.01.065
M3 - Article
AN - SCOPUS:84873333968
SN - 0378-7753
VL - 232
SP - 219
EP - 223
JO - Journal of Power Sources
JF - Journal of Power Sources
ER -