TY - JOUR
T1 - Oxidation ablation resistance of ZrB2-HfB2-SiC-TaSi2 coating prepared on C/C composite surface
AU - Wang, Yifan
AU - Liu, Yanbo
AU - Ma, Zhuang
AU - Zhu, Shizhen
AU - Liu, Ling
AU - Xie, Mingshao
AU - Zhang, Ze
AU - Wang, Ruiqiang
N1 - Publisher Copyright:
© 2023
PY - 2023/8/15
Y1 - 2023/8/15
N2 - In order to improve the oxidation and ablative properties of C/C composites, ZrB2-SiC-HfB2-TaSi2 coating was prepared on the surface of C/C composites by atmospheric plasma spraying. By means of microstructure analysis and phase structure analysis, the difference of the spray powder before and after IPS treatment and the microstructure and oxidation ablation resistance of the coating were studied. The results show that the IPS treated powder has better fluidity and densification. In the coating, part of ZrB2 and HfB2 exist in the form of unmelted particles, another part exists in the form of intermediate solid solution (Zr, Hf)B2, and TaSi2 exists in the particle gap. The linear ablation rate and mass ablation rate of the coating are −1.513 × 10−4 mm/s and 2.842 × 10−4 g/s, respectively, measured under the condition of oxygen acetylene heat flux of 1.8 MW/m2, 180 s were ablated. The coating has good ablative resistance, and TaSi2 can form dense Zr-Ta-O and Hf-Ta-O oxides with Zr and Hf elements. The Ta-Si-O glass phase can effectively seal the holes of the coating to prevent oxygen penetration. During the ablation process, the oxidation of (Zr,Hf)B2 also plays a certain role in the formation of densification zone on the coating surface.
AB - In order to improve the oxidation and ablative properties of C/C composites, ZrB2-SiC-HfB2-TaSi2 coating was prepared on the surface of C/C composites by atmospheric plasma spraying. By means of microstructure analysis and phase structure analysis, the difference of the spray powder before and after IPS treatment and the microstructure and oxidation ablation resistance of the coating were studied. The results show that the IPS treated powder has better fluidity and densification. In the coating, part of ZrB2 and HfB2 exist in the form of unmelted particles, another part exists in the form of intermediate solid solution (Zr, Hf)B2, and TaSi2 exists in the particle gap. The linear ablation rate and mass ablation rate of the coating are −1.513 × 10−4 mm/s and 2.842 × 10−4 g/s, respectively, measured under the condition of oxygen acetylene heat flux of 1.8 MW/m2, 180 s were ablated. The coating has good ablative resistance, and TaSi2 can form dense Zr-Ta-O and Hf-Ta-O oxides with Zr and Hf elements. The Ta-Si-O glass phase can effectively seal the holes of the coating to prevent oxygen penetration. During the ablation process, the oxidation of (Zr,Hf)B2 also plays a certain role in the formation of densification zone on the coating surface.
KW - Atmospheric plasma spraying
KW - C/C composites
KW - Ultra-high temperature ceramic coating
KW - ZrB-SiC-HfB-TaSi coating
UR - http://www.scopus.com/inward/record.url?scp=85159366445&partnerID=8YFLogxK
U2 - 10.1016/j.surfcoat.2023.129615
DO - 10.1016/j.surfcoat.2023.129615
M3 - Article
AN - SCOPUS:85159366445
SN - 0257-8972
VL - 466
JO - Surface and Coatings Technology
JF - Surface and Coatings Technology
M1 - 129615