Indentation creep tests to assess the viscoelastic properties of soft materials: Theory, method and experiment

Xiao Zhang, Yang Zheng, Guo Yang Li, Yan Lin Liu, Yanping Cao*

*此作品的通讯作者

科研成果: 期刊稿件文章同行评审

9 引用 (Scopus)
Plum Print visual indicator of research metrics
  • Citations
    • Citation Indexes: 9
  • Captures
    • Readers: 19
see details

摘要

Determining time-dependent mechanical properties of soft materials is essential in understanding their deformation behaviors under various stimuli. This paper investigates the use of indentation creep tests to measure the viscoelastic properties of soft materials at local areas. A simple scaling law between the reduced creep function and the creep displacement of the indenter is revealed in this paper based on a theoretical analysis. We show that the scaling relation can be used to interpret indentation creep tests of viscoelastic soft solids with arbitrary surface profile provided that the contact area does not change. Both numerical and practical experiments have been performed to validate the theory and the analytical solution. In our experiments, a low-cost portable indentation system is proposed to measure the reduced creep function. Our results show that the low-cost instrument and the analytical solution to interpret the experimental data reported here represent a useful testing method to deduce the intrinsic viscoelastic properties of soft materials in a non-destructive manner.

源语言英语
页(从-至)204-212
页数9
期刊International Journal of Non-Linear Mechanics
109
DOI
出版状态已出版 - 3月 2019
已对外发布

指纹

探究 'Indentation creep tests to assess the viscoelastic properties of soft materials: Theory, method and experiment' 的科研主题。它们共同构成独一无二的指纹。

引用此

Zhang, X., Zheng, Y., Li, G. Y., Liu, Y. L., & Cao, Y. (2019). Indentation creep tests to assess the viscoelastic properties of soft materials: Theory, method and experiment. International Journal of Non-Linear Mechanics, 109, 204-212. https://doi.org/10.1016/j.ijnonlinmec.2018.12.005