TY - JOUR
T1 - Hot-wire arc additive manufacturing of aluminum alloy with reduced porosity and high deposition rate
AU - Fu, Rui
AU - Tang, Shuiyuan
AU - Lu, Jiping
AU - Cui, Yinan
AU - Li, Zixiang
AU - Zhang, Haorui
AU - Xu, Tianqiu
AU - Chen, Zhuo
AU - Liu, Changmeng
N1 - Publisher Copyright:
© 2020 The Author(s)
PY - 2021/2/1
Y1 - 2021/2/1
N2 - Wire arc additive manufacturing (WAAM) technology has attracted considerable interest in large-scale metallic components, but porosity and low deposition rate are the two dominating technical challenges in WAAM of aluminum alloy. In order to effectively solve these problems, a novel method of hot-wire arc additive manufacturing is used to fabricate aluminum alloy. Systematic studies are carried out to investigate the formation mechanism of the pores, the macro/microstructures, as well as the mechanical properties of the parts. It is found that the pores were mainly clustered at the inter-layer. With the increase of the hot-wire current, the porosity firstly decreases, then reaches a minimum at 100 A, and afterwards increases progressively. The corresponding density changes from 96.8% at the hot-wire current of 0 A to 99.6% at 100 A. Increasing the current from 0 A to 120 A also leads to the increase of the deposition rate by about 3.5 times, and the gradual increase of the size of equiaxed grain by 1.6 times. The mechanical properties are considerably improved with the decrease of the porosity.
AB - Wire arc additive manufacturing (WAAM) technology has attracted considerable interest in large-scale metallic components, but porosity and low deposition rate are the two dominating technical challenges in WAAM of aluminum alloy. In order to effectively solve these problems, a novel method of hot-wire arc additive manufacturing is used to fabricate aluminum alloy. Systematic studies are carried out to investigate the formation mechanism of the pores, the macro/microstructures, as well as the mechanical properties of the parts. It is found that the pores were mainly clustered at the inter-layer. With the increase of the hot-wire current, the porosity firstly decreases, then reaches a minimum at 100 A, and afterwards increases progressively. The corresponding density changes from 96.8% at the hot-wire current of 0 A to 99.6% at 100 A. Increasing the current from 0 A to 120 A also leads to the increase of the deposition rate by about 3.5 times, and the gradual increase of the size of equiaxed grain by 1.6 times. The mechanical properties are considerably improved with the decrease of the porosity.
KW - 2024 alloy
KW - Deposition rate
KW - Hot-wire arc additive manufacturing
KW - Macro/microstructures
KW - Mechanical properties
KW - Pores
UR - http://www.scopus.com/inward/record.url?scp=85098455279&partnerID=8YFLogxK
U2 - 10.1016/j.matdes.2020.109370
DO - 10.1016/j.matdes.2020.109370
M3 - Article
AN - SCOPUS:85098455279
SN - 0264-1275
VL - 199
JO - Materials and Design
JF - Materials and Design
M1 - 109370
ER -