TY - JOUR
T1 - Facile preparation of ladder aluminosilsesquioxanes with high flame retardancy for polycarbonate
AU - Wu, Xiaolu
AU - Zhang, Wenchao
AU - Qin, Zhaolu
AU - Yang, Rongjie
N1 - Publisher Copyright:
© 2024
PY - 2024/4
Y1 - 2024/4
N2 - A ladder aluminosilsesquioxanes (Al-L-PPSQ) was synthesized using AlCl3 as an auxiliary catalyst. The chemical structure of Al-L-PPSQ was confirmed by FTIR, 1H, 13C, 29Si-NMR, and MALDI-TOF MS. The well characterized Al-L-PPSQ was used for flame retardant polycarbonate (PC), and the PC/Al-L-PPSQ composite with 6 wt.% Al-L-PPSQ reached UL-94 V-0 rating (1.6 mm), with an oxygen index of 36.6 % and a decrease of 61.2 % in p-HRR. The smoke release of composite materials has also decreased. By analyzing the condensed and gaseous products during the thermal degradation process of PC/Al-L-PPSQ composite materials, it is demonstrated that Al-L-PPSQ can promote the early decomposition of PC into carbon and quickly form a stable and dense char layer to protect the internal substrate during combustion, thereby improving the flame retardancy of PC.
AB - A ladder aluminosilsesquioxanes (Al-L-PPSQ) was synthesized using AlCl3 as an auxiliary catalyst. The chemical structure of Al-L-PPSQ was confirmed by FTIR, 1H, 13C, 29Si-NMR, and MALDI-TOF MS. The well characterized Al-L-PPSQ was used for flame retardant polycarbonate (PC), and the PC/Al-L-PPSQ composite with 6 wt.% Al-L-PPSQ reached UL-94 V-0 rating (1.6 mm), with an oxygen index of 36.6 % and a decrease of 61.2 % in p-HRR. The smoke release of composite materials has also decreased. By analyzing the condensed and gaseous products during the thermal degradation process of PC/Al-L-PPSQ composite materials, it is demonstrated that Al-L-PPSQ can promote the early decomposition of PC into carbon and quickly form a stable and dense char layer to protect the internal substrate during combustion, thereby improving the flame retardancy of PC.
KW - Aluminosilsesquioxanes
KW - Aluminum chloride
KW - Flame retardant
KW - Polycarbonate
UR - http://www.scopus.com/inward/record.url?scp=85187544377&partnerID=8YFLogxK
U2 - 10.1016/j.polymdegradstab.2024.110694
DO - 10.1016/j.polymdegradstab.2024.110694
M3 - Article
AN - SCOPUS:85187544377
SN - 0141-3910
VL - 222
JO - Polymer Degradation and Stability
JF - Polymer Degradation and Stability
M1 - 110694
ER -