T1 - Effect of Yb2O3 Addition and Sintering Temperature on the Densification Behavior of Magnesium Aluminate Spinel Powder
AU - Zeng, Siya
AU - Xiang, Yuan
AU - Liu, Jianhua
AU - Zhou, Junwen
AU - Wang, Guangping
AU - Huang, Ziming
N1 - Publisher Copyright:
© 2024 Indian Ceramic Society.
PY - 2024
Y1 - 2024
N2 - The effect of Yb2O3 and sintering temperature on the densification behavior of magnesium aluminate spinel powder was studied. Results showed that Yb2O3 was beneficial to the sintering densification of MgAl2O4. When the content of Yb2O3 was 3 wt%, the relative density of magnesium aluminium spinel (MAS) was 98.54%, and the microstructure was more compact. The maximum hardness was 21.48 GPa, and the second phase Yb3Al5O12 appeared in the 3 wt% Yb2O3 samples. The mechanism of Yb2O3 in promoting the sintering densification of MAS is due to the appearance of Yb3Al5O12. When the sintering temperature is 1700°C, the relative density of MAS reaches a maximum of 98.54%, the hardness also reaches a maximum value of 21.48 GPa, and the grain size is more uniform. When the temperature exceeds 1700°C, the relative density and hardness of MAS decrease. The best sintering aid content and temperature synergistically worked to promote the densification and increased the hardness of MAS.
AB - The effect of Yb2O3 and sintering temperature on the densification behavior of magnesium aluminate spinel powder was studied. Results showed that Yb2O3 was beneficial to the sintering densification of MgAl2O4. When the content of Yb2O3 was 3 wt%, the relative density of magnesium aluminium spinel (MAS) was 98.54%, and the microstructure was more compact. The maximum hardness was 21.48 GPa, and the second phase Yb3Al5O12 appeared in the 3 wt% Yb2O3 samples. The mechanism of Yb2O3 in promoting the sintering densification of MAS is due to the appearance of Yb3Al5O12. When the sintering temperature is 1700°C, the relative density of MAS reaches a maximum of 98.54%, the hardness also reaches a maximum value of 21.48 GPa, and the grain size is more uniform. When the temperature exceeds 1700°C, the relative density and hardness of MAS decrease. The best sintering aid content and temperature synergistically worked to promote the densification and increased the hardness of MAS.
KW - Densification
KW - Hardness
KW - Magnesium aluminate spinel
KW - Sintering temperature
KW - YbO
UR - http://www.scopus.com/inward/record.url?scp=85197378254&partnerID=8YFLogxK
U2 - 10.1080/0371750X.2024.2351944
DO - 10.1080/0371750X.2024.2351944
M3 - Article
AN - SCOPUS:85197378254
SN - 0371-750X
VL - 83
SP - 134
EP - 139
JO - Transactions of the Indian Ceramic Society
JF - Transactions of the Indian Ceramic Society
IS - 2
ER -