TY - JOUR
T1 - Effect of processing parameters on the microstructure and mechanical properties of TiAl/Ti2AlNb laminated composites
AU - Li, Donghai
AU - Wang, Binbin
AU - Luo, Liangshun
AU - Li, Xuewen
AU - Xu, Yanjin
AU - Li, Bin Qiang
AU - Hawezy, Diween
AU - Wang, Liang
AU - Su, Yanqing
AU - Guo, Jingjie
AU - Fu, Hengzhi
N1 - Publisher Copyright:
© 2021
PY - 2022/5/20
Y1 - 2022/5/20
N2 - In order to improve the intrinsic brittleness of TiAl alloys, Ti2AlNb alloys with outstanding ductility and toughness at room temperature, and good high-temperature performance are competitive candidates in constructing the TiAl-based laminated composites. In this work, TiAl/Ti2AlNb laminated composites are successfully synthesized by vacuum hot pressing combined with the foil-foil (sheet) metallurgy. Under the pressure of 65 MPa, different holding time and temperature of hot pressing are tried and the optimized fabrication parameter is acquired as 1050 °C/120 min/65 MPa. Along with the changes of processing parameters, the defect, microstructure, interface, phase transformation and the corresponding mechanical properties are detailly discussed. The results show that the TiAl/Ti2AlNb laminated composite fabricated at 1050 °C for 2 h achieves a good metallurgical interface bonding. The corresponding interface microstructure is composed of region I and region II. The region I consists of O, α2 and B2/β phase, and region II is made up of α2. Subsequently, the tensile tests indicate that the composite synthesized at 1050 °C for 2 h possesses a maximum strength of 812 MPa and a total elongation of 1.31% at room temperature, and a strength of 539.71 MPa and the highest total elongation of 10.34% at 750 °C. The well synergistic deformation ability between the interface and the two base alloys endows the composite an excellent tensile performance. Moreover, the composite processed at 1050 °C for 2 h behaves the best fracture toughness in both arrester orientation and divider orientation with the value of 32.6 MPa.m1/2 and 30.1 MPa.m1/2, respectively. The Ti2AlNb alloy in the laminated structure effectively release the stress around the crack tip and plays a role in toughening. Further, crack deflection, crack bridging, crack blunting and fragmentation also make contributions to enhance the fracture toughness of the laminated composites.
AB - In order to improve the intrinsic brittleness of TiAl alloys, Ti2AlNb alloys with outstanding ductility and toughness at room temperature, and good high-temperature performance are competitive candidates in constructing the TiAl-based laminated composites. In this work, TiAl/Ti2AlNb laminated composites are successfully synthesized by vacuum hot pressing combined with the foil-foil (sheet) metallurgy. Under the pressure of 65 MPa, different holding time and temperature of hot pressing are tried and the optimized fabrication parameter is acquired as 1050 °C/120 min/65 MPa. Along with the changes of processing parameters, the defect, microstructure, interface, phase transformation and the corresponding mechanical properties are detailly discussed. The results show that the TiAl/Ti2AlNb laminated composite fabricated at 1050 °C for 2 h achieves a good metallurgical interface bonding. The corresponding interface microstructure is composed of region I and region II. The region I consists of O, α2 and B2/β phase, and region II is made up of α2. Subsequently, the tensile tests indicate that the composite synthesized at 1050 °C for 2 h possesses a maximum strength of 812 MPa and a total elongation of 1.31% at room temperature, and a strength of 539.71 MPa and the highest total elongation of 10.34% at 750 °C. The well synergistic deformation ability between the interface and the two base alloys endows the composite an excellent tensile performance. Moreover, the composite processed at 1050 °C for 2 h behaves the best fracture toughness in both arrester orientation and divider orientation with the value of 32.6 MPa.m1/2 and 30.1 MPa.m1/2, respectively. The Ti2AlNb alloy in the laminated structure effectively release the stress around the crack tip and plays a role in toughening. Further, crack deflection, crack bridging, crack blunting and fragmentation also make contributions to enhance the fracture toughness of the laminated composites.
KW - Fracture
KW - Hot pressing
KW - Mechanical properties
KW - Microstructure
KW - Processing parameters
KW - TiAl/TiAlNb laminated composite
UR - http://www.scopus.com/inward/record.url?scp=85119081336&partnerID=8YFLogxK
U2 - 10.1016/j.jmst.2021.08.067
DO - 10.1016/j.jmst.2021.08.067
M3 - Article
AN - SCOPUS:85119081336
SN - 1005-0302
VL - 109
SP - 228
EP - 244
JO - Journal of Materials Science and Technology
JF - Journal of Materials Science and Technology
ER -