The authors regret that a label in figure 7(b) was not correctly presented, namely, the sample names of “Bare Li” and “LiF-rich Li” should be switched. The correct figure should be revised as below: [Figure presented] The authors would like to apologize for any inconvenience caused.
源语言 | 英语 |
---|---|
页(从-至) | 386 |
页数 | 1 |
期刊 | Energy Storage Materials |
卷 | 29 |
DOI |
|
出版状态 | 已出版 - 8月 2020 |
指纹
探究 'Corrigendum for “Regulating Li deposition by constructing LiF-rich host for dendrite-free lithium metal anode” [Energy Storage Mater. 16 (2019) 411-418] (Energy Storage Materials (2019) 16 (411-418), (S2405829718302125), (10.1016/j.ensm.2018.06.022))' 的科研主题。它们共同构成独一无二的指纹。引用此
Yuan, Y., Wu, F., Bai, Y., Li, Y., Chen, G., Wang, Z., & Wu, C. (2020). Corrigendum for “Regulating Li deposition by constructing LiF-rich host for dendrite-free lithium metal anode” [Energy Storage Mater. 16 (2019) 411-418] (Energy Storage Materials (2019) 16 (411-418), (S2405829718302125), (10.1016/j.ensm.2018.06.022)). Energy Storage Materials, 29, 386. https://doi.org/10.1016/j.ensm.2020.03.028