摘要
The forming mechanism of Sm2Zr2O7 prepared by solid reaction was studied by X-Ray diffraction method. The results show that the gradual substitution of Sm3+ for Zr4+ site began from 1000°C. and was ended basically up to 1400°C. The solid solution reaction between Sm2O3 and ZrO2 took place in the range of 1200°C-1300°C, resulting in forming Sm2Zr2O7 with pyrochlore structure. The reaction last up to 1500°C, then was ended completely. When the temperature was over 1500°C, Sm2Zr2O7 crystal grew up gradually, and finally an ideal Sm2Zr2O7 crystal was obtained. No other intermediate phases were found in the whole process.