摘要

Strategies for protecting unstable semiconductors include the utilization of surface layers composed of thin films deposited using atomic layer deposition (ALD). The protective layer is expected to (1) be stable against reaction with photogenerated holes, (2) prevent direct contact of the unstable semiconductor with the electrolyte, and (3) prevent the migration of ions through the semiconductor/electrolyte interface, while still allowing photogenerated carriers to transport to the interface and participate in the desired redox reactions. Zinc oxide (ZnO) is an attractive photocatalyst material due to its high absorption coefficient and high carrier mobilities. However, ZnO is chemically unstable and undergoes photocorrosion, which limits its use in applications such as in photoelectrochemical cells for water splitting or photocatalytic water purification. This article describes an investigation of the band alignment, electrochemical properties, and interfacial structure of ZnO coated with Al2O3 and SiO2 ALD layers. The interface electronic properties were determined using in situ X-ray and UV photoemission spectroscopy, and the photochemical response and stability under voltage bias were determined using linear sweep voltammetry and chronoamperometry. The resulting surface structure and degradation processes were identified using atomic force, scanning electron, and transmission electron microscopy. The suite of characterization tools enable the failure mechanisms to be more clearly discerned. The results show that the rapid photocorrosion of ZnO thin films is only slightly slowed by use of an Al2O3 ALD coating. A 4 nm SiO2 layer proved to be more effective, but its protection capability could be affected by the diffusion of ions from the electrolyte.

源语言英语
页(从-至)16138-16147
页数10
期刊ACS applied materials & interfaces
9
19
DOI
出版状态已出版 - 17 5月 2017
已对外发布

指纹

探究 'Al2O3 and SiO2 Atomic Layer Deposition Layers on ZnO Photoanodes and Degradation Mechanisms' 的科研主题。它们共同构成独一无二的指纹。

引用此

Cheng, Q., Benipal, M. K., Liu, Q., Wang, X., Crozier, P. A., Chan, C. K., & Nemanich, R. J. (2017). Al2O3 and SiO2 Atomic Layer Deposition Layers on ZnO Photoanodes and Degradation Mechanisms. ACS applied materials & interfaces, 9(19), 16138-16147. https://doi.org/10.1021/acsami.7b01274