摘要
Morphological degradation at the Li/solid-state electrolyte (SSE) interface is a prevalent issue causing performance fading of all-solid-state batteries (ASSBs). To maintain the interfacial integrity, most ASSBs are operated under low current density with considerable stack pressure, which significantly limits their widespread usage. Herein, a novel 3D-micropatterned SSE (3D-SSE) that can stabilize the morphology of the Li/SSE interface even under relatively high current density and limited stack pressure is reported. Under the pressure of 1.0 MPa, the Li symmetric cell using a garnet-type 3D-SSE fabricated by laser machining shows a high critical current density of 0.7 mA cm–2 and stable cycling over 500 h under 0.5 mA cm–2. This excellent performance is attributed to the reduced local current density and amplified mechanical stress at the Li/3D-SSE interface. These two effects can benefit the flux balance between Li stripping and creep at the interface, thereby preventing interfacial degradation such as void formation and dendrite growth.
源语言 | 英语 |
---|---|
文章编号 | 2104009 |
期刊 | Advanced Materials |
卷 | 33 |
期 | 49 |
DOI | |
出版状态 | 已出版 - 9 12月 2021 |
已对外发布 | 是 |