Standing and sitting adlayers in atomic layer deposition of ZnO

Zhengning Gao, Fei Wu, Yoon Myung, Ruixiang Fei, Ravindra Kanjolia, Li Yang, Parag Banerjee

Research output: Contribution to journalArticlepeer-review

21 Citations (Scopus)
Plum Print visual indicator of research metrics
  • Citations
    • Citation Indexes: 21
  • Captures
    • Readers: 19
see details

Abstract

The extent of reactivity of diethyl zinc (DEZ) with a hydroxylated surface during atomic layer deposition (ALD) of ZnO using DEZ and water is measured. Two adlayer configurations of DEZ are possible. The "standing" adlayer releases one ethyl group from DEZ. The "sitting" adlayer releases both ethyl groups, thus forming a Zn bridge between two O anions. Density functional theory calculations suggest the sitting configuration is more stable than the standing configuration by 790 meV. In situ quadrupole mass spectroscopy of by-product ethane generated in ALD half cycles indicate that ∼1.56 OH sites react with a DEZ molecule resulting in 71.6% of sitting sites. A simple simulation of a "ball-and-stick" DEZ molecule randomly collapsing on a neighboring site remarkably captures this adlayer behavior. It is concluded that DEZ fraction sitting is a competitive process of a standing DEZ molecule collapsing onto an available neighboring hydroxyl site, as sites vie for occupancy via adsorption and surface diffusion.

Original languageEnglish
Article number01A143
JournalJournal of Vacuum Science and Technology A: Vacuum, Surfaces and Films
Volume34
Issue number1
DOIs
Publication statusPublished - 1 Jan 2016
Externally publishedYes

Fingerprint

Dive into the research topics of 'Standing and sitting adlayers in atomic layer deposition of ZnO'. Together they form a unique fingerprint.

Cite this

Gao, Z., Wu, F., Myung, Y., Fei, R., Kanjolia, R., Yang, L., & Banerjee, P. (2016). Standing and sitting adlayers in atomic layer deposition of ZnO. Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films, 34(1), Article 01A143. https://doi.org/10.1116/1.4938080