Abstract
A preparation method of nanoporous silver was introduced. First, polystyrene (PS) was pretreated. Then silver was deposited on the surface of PS. And finally, PS was removed to obtain porous silver by extraction. The effects of different reaction conditions on the reaction rate and silver deposits were studied. The reaction conditions include silver nitrate concentration, sodium hydroxide concentration, glucose concentration and temperature. The best reaction condition is 0.074 mol•L-1 AgNO3, 0.22 mol•L-1 glucose, 0.05mol•L-1 NaOH and the reaction temperature is 20°C.
Original language | English |
---|---|
Article number | 012030 |
Journal | Journal of Physics: Conference Series |
Volume | 1838 |
Issue number | 1 |
DOIs | |
Publication status | Published - 26 Mar 2021 |
Event | 8th Annual International Conference on Material Science and Environmental Engineering, MSEE 2020 - Chengdu, Sichuan, Virtual, China Duration: 20 Nov 2020 → 21 Nov 2020 |
Fingerprint
Dive into the research topics of 'Preparation of Nano-Porous Silver by Electroless Plating'. Together they form a unique fingerprint.Cite this
Ban, B., Li, M., & Zeng, Q. (2021). Preparation of Nano-Porous Silver by Electroless Plating. Journal of Physics: Conference Series, 1838(1), Article 012030. https://doi.org/10.1088/1742-6596/1838/1/012030