Preparation and dielectric property of SiO2 surface coating modified BaTiO3/polyimide composite film

Ya Jun Wang*, Xiao Juan Wu, Chang Gen Feng, Qing Xuan Zeng

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

1 Citation (Scopus)

Abstract

Polyimide (PI) was chosen as the matrix of the composite, barium titanate/polyimide (BaTiO3/PI) nanocomposite films were prepared with in situ polymerization. In order to improve the dispersion and the physical-chemical properties of BT surface, barium titanate was modified by SiO2 coating and modified barium titanate/polyimide (BaTiO3/PI) nanocomposite films were prepared. The prepared modified BaTiO3 was characterized by X-ray diffraction (XRD) analysis, Fourier transform infrared spectroscopy (FT-IR) and scanning electron microscopy (SEM), and the dielectric properties of the composites were characterized in detail. It was shown that surface modification with SiO2 was the physical effect and there were no new substances forming. When BaTiO3 was modified by 5% SiO2, the dielectric constant of the composite film was 21.8 (103 Hz), the loss tangent 0.00521, breakdown strength 76 MV/m, energy storage density 0.56 J/cm3. The BaTiO3 surface coating modification by SiO2 was beneficial to the dielectric properties of the BaTiO3/PI composite film.

Original languageEnglish
Pages (from-to)1066-1069
Number of pages4
JournalGongneng Cailiao/Journal of Functional Materials
Volume46
Issue number1
DOIs
Publication statusPublished - 15 Jan 2015

Keywords

  • Dielectric constant
  • Nanometer barium titanate
  • Polyimide
  • Storage energy density
  • Surface coating modification