TY - JOUR
T1 - Erratum
T2 - Overcharge investigation of large format lithium-ion pouch cells with Li(Ni0.6Co0.2Mn0.2)O2 cathode for electric vehicles: Degradation and failure mechanisms (J. Electrochem. Soc. (2018) 165 (A3613) DOI: 10.1149/2.0161816jes)
AU - Zhu, Xiaoqing
AU - Wang, Zhenpo
AU - Wang, Cong
AU - Huang, Lvwei
N1 - Publisher Copyright:
© 2018 The Electrochemical Society.
PY - 2018
Y1 - 2018
N2 - The caption for Fig. 12 on page A3627 should read as follows: Figure 12. The failure mechanism of overcharge-to-thermal runaway process at each stage as reported in Refs. 69, 72, and 73. The references listed on page A3629 should include the following: 73. D. Ren, X. Feng, L. Lu, M. Ouyang, S. Zheng, J. Li, and X. He, J. Power Sources, 364, 328 (2017).
AB - The caption for Fig. 12 on page A3627 should read as follows: Figure 12. The failure mechanism of overcharge-to-thermal runaway process at each stage as reported in Refs. 69, 72, and 73. The references listed on page A3629 should include the following: 73. D. Ren, X. Feng, L. Lu, M. Ouyang, S. Zheng, J. Li, and X. He, J. Power Sources, 364, 328 (2017).
UR - http://www.scopus.com/inward/record.url?scp=85067472263&partnerID=8YFLogxK
U2 - 10.1149/2.0551816jes
DO - 10.1149/2.0551816jes
M3 - Comment/debate
AN - SCOPUS:85067472263
SN - 0013-4651
VL - 165
SP - X21
JO - Journal of the Electrochemical Society
JF - Journal of the Electrochemical Society
IS - 16
ER -