TY - JOUR
T1 - Enhancing Flame Retardancy and Thermal Insulation Performance of Silicone Rubber Composites Using Silicon Carbide
AU - Lou, Xu
AU - Zang, Chongguang
AU - Pan, Hongwei
N1 - Publisher Copyright:
© 2024 Institute of Physics Publishing. All rights reserved.
PY - 2024
Y1 - 2024
N2 - This study focuses on modifying silicone rubber using silicon carbide (SiC) to enhance the flame retardancy and thermal insulation properties of the composites. The study characterizes the thermal stability, mechanical properties, and flame retardancy of the composite materials. The results demonstrate the effective improvement in thermal stability achieved by incorporating SiC into the silicone rubber composites. At a SiC addition level of 6 wt.%, the composite material shows optimal thermal stability with an initial decomposition temperature of 487°C, which is 84°C higher compared to the pure matrix. Additionally, the SiC/SR composites system exhibits a char yield of 72.13% at 900°C, representing an approximately 9% increase compared to the pure SR matrix. Simultaneously, the incorporation of SiC significantly enhances the flame retardancy of silicone rubber. At a SiC addition level of 10 wt.%, the LOI (Limiting Oxygen Index) value increases by 10.5% to reach 30.4%, surpassing the non-additive sample. Moreover, the UL-94 classification of the composite material is V-0, meeting the standard for flame retardant materials.
AB - This study focuses on modifying silicone rubber using silicon carbide (SiC) to enhance the flame retardancy and thermal insulation properties of the composites. The study characterizes the thermal stability, mechanical properties, and flame retardancy of the composite materials. The results demonstrate the effective improvement in thermal stability achieved by incorporating SiC into the silicone rubber composites. At a SiC addition level of 6 wt.%, the composite material shows optimal thermal stability with an initial decomposition temperature of 487°C, which is 84°C higher compared to the pure matrix. Additionally, the SiC/SR composites system exhibits a char yield of 72.13% at 900°C, representing an approximately 9% increase compared to the pure SR matrix. Simultaneously, the incorporation of SiC significantly enhances the flame retardancy of silicone rubber. At a SiC addition level of 10 wt.%, the LOI (Limiting Oxygen Index) value increases by 10.5% to reach 30.4%, surpassing the non-additive sample. Moreover, the UL-94 classification of the composite material is V-0, meeting the standard for flame retardant materials.
UR - http://www.scopus.com/inward/record.url?scp=85188271083&partnerID=8YFLogxK
U2 - 10.1088/1742-6596/2706/1/012003
DO - 10.1088/1742-6596/2706/1/012003
M3 - Conference article
AN - SCOPUS:85188271083
SN - 1742-6588
VL - 2706
JO - Journal of Physics: Conference Series
JF - Journal of Physics: Conference Series
IS - 1
M1 - 012003
T2 - 11th Annual International Conference on Material Science and Environmental Engineering, MSEE 2023
Y2 - 24 November 2023 through 26 November 2023
ER -