Eliminating interfacial O-involving degradation in Li-rich Mn-based cathodes for all-solid-state lithium batteries

Shuo Sun, Chen Zi Zhao*, Hong Yuan, Zhong Heng Fu, Xiang Chen, Yang Lu, Yun Fan Li, Jiang Kui Hu, Juncai Dong, Jia Qi Huang, Minggao Ouyang, Qiang Zhang*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

106 Citations (Scopus)

Abstract

In the pursuit of energy-dense all-solid-state lithium batteries (ASSBs), Li-rich Mn-based oxide (LRMO) cathodes provide an exciting path forward with unexpectedly high capacity, low cost, and excellent processibility. However, the cause for LRMO|solid electrolyte interfacial degradation remains a mystery, hindering the application of LRMO-based ASSBs. Here, we first reveal that the surface oxygen instability of LRMO is the driving force for interfacial degradation, which severely blocks the interfacial Li-ion transport and triggers fast battery failure. By replacing the charge compensation of surface oxygen with sulfite, the overoxidation and interfacial degradation can be effectively prevented, therefore achieving a high specific capacity (~248 mAh g−1, 1.1 mAh cm−2; ~225 mAh g−1, 2.9 mAh cm−2) and excellent long-term cycling stability of >300 cycles with 81.2% capacity retention at room temperature. These findings emphasize the importance of irreversible anion reactions in interfacial failure and provide fresh insights into constructing stable interfaces in LRMO-based ASSBs.

Original languageEnglish
Article numbereadd5189
JournalScience advances
Volume8
Issue number47
DOIs
Publication statusPublished - Nov 2022

Fingerprint

Dive into the research topics of 'Eliminating interfacial O-involving degradation in Li-rich Mn-based cathodes for all-solid-state lithium batteries'. Together they form a unique fingerprint.

Cite this