Due to the lack of surface dangling bonds of 2D materials such as graphene, hexagonal boron nitride, MoS2 etc., deposition of high-κ dielectrics directly on such 2D materials by atomic layer deposition (ALD) is difficult and a nucleation layer is usually required. Here an ALD approach is developed to deposit high-κ dielectric layer, e.g., Al2O3, directly on 2D materials without the aid of the nucleation layer or introducing structural damages. In this approach, an individual deposition cycle includes one incremental organometallic pulse and multiple H2O pulses to guarantee the uniform deposition of high-quality high-κ dielectric layers on graphene, MoS2, and other 2D materials directly. Large-scale top-gated MoS2 field-effect transistors (FETs) with Al2O3 as dielectric layers exhibit excellent performances including high on/off ratio exceeding 108 and mobility up to 70 cm2 V−1 s−1. The high-quality Al2O3 layer is also integrated into MoS2 based flexible FETs and inverters, and a significant voltage gain of 412 is obtained. This ALD approach also works for other materials like gold with inert surfaces, showing great promise for novel electronics.

Original languageEnglish
Article number1802055
JournalAdvanced Materials Interfaces
Volume6
Issue number10
DOIs
Publication statusPublished - 23 May 2019
Externally publishedYes

Keywords

  • 2D materials
  • atomic layer deposition
  • flexible electronics
  • high-κ
  • top-gate FETs

Fingerprint

Dive into the research topics of 'Atomic Layer Deposition of Al2O3 Directly on 2D Materials for High-Performance Electronics'. Together they form a unique fingerprint.

Cite this