A zero-strain Na-deficient NASICON-type Na2.8Mn0.4V1.0Ti0.6(PO4)3 cathode for wide-temperature rechargeable Na-ion batteries

Xing Shen, Yuefeng Su*, Shunli He, Yali Li, Lifeng Xu, Ni Yang, Yanshun Liao, Meng Wang, Feng Wu*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

7 Citations (Scopus)

Abstract

Na superionic conductor (NASICON) type cathode materials with high structural stability and fast Na+ diffusion have been considered as high-power candidates for the exploration of Na-ion batteries. However, the substitution of active elements with low cost and additional attributes remains epoch-making due to the structural flexibility and insufficient utilization of the introduced components. Herein, the Na-deficient strategy based on charge balance is employed to take full advantage of the Na+ ions and active transition metals within the voltage window of 2.0-4.2 V. The optimized Na2.8Mn0.4V1.0Ti0.6(PO4)3 cathode realizes a 2.1 e redox reaction with a 76% utilization rate of Na+ ions rooted in the lattice, allowing a discharge capacity of 126.2 mA h g−1 and superior capacity retention of 88.1% at 20 C over 3000 cycles. Consequently, the developed cathode also achieved superior reaction reversibility and remarkable Na-storage properties, even under extreme working conditions and with full cell configurations. This work could provide new perspectives and an efficient regulation protocol for high-performance Na-ion batteries.

Original languageEnglish
Pages (from-to)16860-16870
Number of pages11
JournalJournal of Materials Chemistry A
Volume11
Issue number31
DOIs
Publication statusPublished - 15 Jul 2023

Fingerprint

Dive into the research topics of 'A zero-strain Na-deficient NASICON-type Na2.8Mn0.4V1.0Ti0.6(PO4)3 cathode for wide-temperature rechargeable Na-ion batteries'. Together they form a unique fingerprint.