TY - JOUR
T1 - Valorization of hazardous phosphating sludge
T2 - construction of a carbon-rich, heterointerfacial, halogen-free and all-in-one flame retardant for silicone rubber
AU - Zhang, Ziyang
AU - Wang, Wen
AU - Guo, Xiaoyang
AU - He, Jing
AU - Xu, Junwen
AU - Zheng, Zaihang
AU - Pan, Ye Tang
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/12/15
Y1 - 2026/12/15
N2 - Silicone rubber (SR) was widely used in fire-sensitive applications, but its inherent flammability remained a major limitation. Conventional flame-retardant modification often relied on a high loading of inorganic additives or multi-component intumescent system, which might cause poor interfacial compatibility, high filler demand, and deterioration of mechanical strength. Meanwhile, hazardous phosphating sludge generated from automotive pretreatment process was a disposal-restricted industrial by-product rich in inorganic phosphates and metal oxide phases, making it a potentially useful inorganic component for flame-retardant structural design and waste valorization. In this work, a single-component integrated flame retardant (Si-WR@MS@DTMA) was prepared through a multistage assembly strategy. Phosphating waste residue (WR) was used as an inorganic skeleton, a hydroxyethyl-cellulose-derived carbonaceous interlayer was constructed on its surface, a melamine/diethylenetriamine penta(methylene phosphonic acid)-derived phosphorus‑nitrogen layer was subsequently deposited, and epoxy-modified silicone resin (EPSR) was introduced for interfacial regulation. With 25 phr Si-WR@MS@DTMA, the resulting SR composite exhibited a LOI of 29.5%, achieved a UL-94 V-0 rating, a pHRR reduction of 42.9% and a THR reduction of 17.2%, respectively. Its glow-wire ignition temperature (GWIT) was increased to 875 ± 25 °C, and the mass loss after 5 min flame impingement test was only 8.0%. The enhanced flame retardancy was associated with inorganic skeletal support, enhanced retention of carbonaceous structures, phosphorus/nitrogen-assisted residue construction, and the suppressed release of combustible cyclic siloxane products. In addition, the Young's modulus was increased by 500%, while the elongation at break remained at 207%. This work provided a feasible strategy for the value-added utilization of industrial solid waste and the design of mechanically reliable flame-retarding SR composites.
AB - Silicone rubber (SR) was widely used in fire-sensitive applications, but its inherent flammability remained a major limitation. Conventional flame-retardant modification often relied on a high loading of inorganic additives or multi-component intumescent system, which might cause poor interfacial compatibility, high filler demand, and deterioration of mechanical strength. Meanwhile, hazardous phosphating sludge generated from automotive pretreatment process was a disposal-restricted industrial by-product rich in inorganic phosphates and metal oxide phases, making it a potentially useful inorganic component for flame-retardant structural design and waste valorization. In this work, a single-component integrated flame retardant (Si-WR@MS@DTMA) was prepared through a multistage assembly strategy. Phosphating waste residue (WR) was used as an inorganic skeleton, a hydroxyethyl-cellulose-derived carbonaceous interlayer was constructed on its surface, a melamine/diethylenetriamine penta(methylene phosphonic acid)-derived phosphorus‑nitrogen layer was subsequently deposited, and epoxy-modified silicone resin (EPSR) was introduced for interfacial regulation. With 25 phr Si-WR@MS@DTMA, the resulting SR composite exhibited a LOI of 29.5%, achieved a UL-94 V-0 rating, a pHRR reduction of 42.9% and a THR reduction of 17.2%, respectively. Its glow-wire ignition temperature (GWIT) was increased to 875 ± 25 °C, and the mass loss after 5 min flame impingement test was only 8.0%. The enhanced flame retardancy was associated with inorganic skeletal support, enhanced retention of carbonaceous structures, phosphorus/nitrogen-assisted residue construction, and the suppressed release of combustible cyclic siloxane products. In addition, the Young's modulus was increased by 500%, while the elongation at break remained at 207%. This work provided a feasible strategy for the value-added utilization of industrial solid waste and the design of mechanically reliable flame-retarding SR composites.
KW - Ablation resistance
KW - Phosphate-rich inorganic waste residue
KW - Silicone rubber
KW - Single-component flame retardant
UR - https://www.scopus.com/pages/publications/105052491699
U2 - 10.1016/j.susmat.2026.e02278
DO - 10.1016/j.susmat.2026.e02278
M3 - Article
AN - SCOPUS:105052491699
SN - 2214-9929
VL - 50
JO - Sustainable Materials and Technologies
JF - Sustainable Materials and Technologies
M1 - e02278
ER -