摘要
Very high cycle fatigue test under pulsating tension was performed to investigate the subsurface failure mechanism of a titanium alloy. A peculiar region, called "facets cluster zone (FCZ)", is located at the center of fisheye. The slip-like patterns on facet surface, coalescence of nanoscale cracks and growth of microcracks in the maximum shear stress plane are observable. Combined with the evaluation of stress intensity factors at crack tips, the subsurface failure processes are summarized as: (a) localization of plastic strain, (b) occurrence of slip lines, (c) nucleation of microcracks, (d) coalescence and growth of microcracks, (f) occurrence of the FCZ, (g) formation of fisheye and (i) unstable crack growth until final fracture.
| 源语言 | 英语 |
|---|---|
| 期刊论文编号 | 012017 |
| 期刊 | IOP Conference Series: Materials Science and Engineering |
| 卷 | 746 |
| 期 | 1 |
| DOI | |
| 出版状态 | 已出版 - 4 3月 2020 |
| 活动 | 2nd Annual International Conference on Mechanical Engineering and Materials, ICMEM 2019 - Guangzhou, 中国 期限: 20 12月 2019 → 21 12月 2019 |
学术指纹
探究 'Subsurface Facet-fisheye Induced Failure of Titanium Alloy under Very High Cycle Fatigue' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver