TY - JOUR
T1 - Regulation of layered grain heterostructure in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing
AU - Liao, Luhui
AU - Duan, Xunan
AU - Zhao, Qian
AU - Sun, Shihai
AU - Liang, Yaojian
AU - Wang, Liang
AU - Xue, Yunfei
N1 - Publisher Copyright:
© 2026, Published under licence by IOP Publishing Ltd. Content from this work may be used under the terms of the Creative Commons Attribution 4.0 licence. Any further distribution of this work must maintain attribution to the author(s) and the title of the work, journal citation and DOI.
PY - 2026
Y1 - 2026
N2 - Heterostructure is a novel microstructure to break the strength and ductility trade-off of materials. In this study, the layered grain heterostructure with tailored grain size and layer thickness was successfully fabricated in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing via alternately modulating the laser process parameters in the adjacent layers. The average grain sizes in the fine and coarse grain layers were ~20 μm and ~53 μm, respectively, and their corresponding layer thicknesses were ~320 μm and ~280 μm under volumetric energy density (VED) of 222 and 167 J/mm3 and scanning speeds of 20 and 15 mm/s, respectively. When the VED was increased to 300 J/mm3, and the scanning speed was lowered to 10 mm/s, the grain size in the fine grain layer could be refined to ~10 μm, and the ratio of the fine and coarse grain sizes reached 1/5, which is expected to induce pronounced hetero-deformation-induced (HDI) strengthening. The grain size refinement is ascribed to the increasing cooling rate at the melt pool boundary at higher VED and lower scanning speed, as suggested by the simulation. The research findings in this paper provide valuable references for the regulation of heterostructures.
AB - Heterostructure is a novel microstructure to break the strength and ductility trade-off of materials. In this study, the layered grain heterostructure with tailored grain size and layer thickness was successfully fabricated in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing via alternately modulating the laser process parameters in the adjacent layers. The average grain sizes in the fine and coarse grain layers were ~20 μm and ~53 μm, respectively, and their corresponding layer thicknesses were ~320 μm and ~280 μm under volumetric energy density (VED) of 222 and 167 J/mm3 and scanning speeds of 20 and 15 mm/s, respectively. When the VED was increased to 300 J/mm3, and the scanning speed was lowered to 10 mm/s, the grain size in the fine grain layer could be refined to ~10 μm, and the ratio of the fine and coarse grain sizes reached 1/5, which is expected to induce pronounced hetero-deformation-induced (HDI) strengthening. The grain size refinement is ascribed to the increasing cooling rate at the melt pool boundary at higher VED and lower scanning speed, as suggested by the simulation. The research findings in this paper provide valuable references for the regulation of heterostructures.
UR - https://www.scopus.com/pages/publications/105052853789
U2 - 10.1088/1742-6596/3254/2/022051
DO - 10.1088/1742-6596/3254/2/022051
M3 - Conference article
AN - SCOPUS:105052853789
SN - 1742-6588
VL - 3254
JO - Journal of Physics: Conference Series
JF - Journal of Physics: Conference Series
IS - 2
M1 - 022051
T2 - 2026 9th International Conference on Mechanical, Electrical and Material Application, MEMA 2026
Y2 - 27 March 2026 through 29 March 2026
ER -