摘要
The porous Fe3O4/carbon core/shell nanorods were fabricated via a three-step process. α-Fe2O3 nanorods were first obtained, and α-Fe2O3/carbon core/shell nanorods were subsequently fabricated using glucose as a carbon source by a hydrothermal method, in which the thickness of the carbon coating was about 3.5 nm. Fe3O4/carbon core/shell nanorods were synthesized after an annealing treatment of the product above under a mixture of Ar/H2 flow. After the H2 deoxidation process, the Fe 3O4 core exhibited a character of porosity; the thickness of the carbon shell was decreased to about 2.5 nm, and its degree of graphitization was enhanced. The interesting core/shell nanostructures are ferromagnetic at room temperature, and the Verwey temperature was about 120 K. Electromagnetic properties of the core/shell nanorod-wax composite were investigated in detail. The maximum reflection loss was about -27.9 dB at 14.96 GHz for the composite with a thickness of 2.0 mm, and the absorption bandwidth with the reflection loss below -18 dB was up to 10.5 GHz for the absorber with the thickness of 2-5 mm. The excellent electromagnetic wave absorption properties of the porous Fe3O4/carbon core/shell nanorods were attributed to effective complementarities between the dielectric loss and the magnetic loss.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 13603-13608 |
| 页数 | 6 |
| 期刊 | Journal of Physical Chemistry C |
| 卷 | 115 |
| 期 | 28 |
| DOI | |
| 出版状态 | 已出版 - 21 7月 2011 |
指纹
探究 'Porous Fe3O4/Carbon core/shell nanorods: Synthesis and electromagnetic properties' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver