TY - JOUR
T1 - Microstructure and mechanical properties of AlN/Al joints vacuum brazed with Al–Si–Mg filler metal
AU - Zhang, Shihan
AU - Wang, Gang
AU - Wang, Wei
AU - Zhao, Yu
AU - He, Rujie
AU - Tan, Caiwang
N1 - Publisher Copyright:
© 2026 Elsevier Ltd and Techna Group S.r.l. All rights are reserved, including those for text and data mining, AI training, and similar technologies.
PY - 2026
Y1 - 2026
N2 - An approximately 1.5 μm-thick Al film was first deposited on the AlN surface by radio-frequency magnetron sputtering, followed by vacuum brazing of the AlN ceramic to an Al substrate using an Al–10.5Si–1.5 Mg(wt.%) filler metal. Brazing was conducted at 550–590 °C for 20 min to investigate the effects of brazing temperature on the joint microstructure, mechanical properties. During cooling, the preferential growth of α-Al rejected Si into the residual liquid, resulting in local Si enrichment within the brazing seam. Among the investigated conditions, the joint brazed at 580 °C exhibited the most uniform brazing seam and achieved the highest shear strength of 55 ± 2 MPa. The 580 °C joint exhibited an effective thermal conductivity of 196.3 W m−1 K−1 at 25 °C. These results demonstrate the feasibility of low-temperature AlN/Al joining using Al metallization and Al–Si–Mg filler metal, with potential applications in electronic thermal-management components.
AB - An approximately 1.5 μm-thick Al film was first deposited on the AlN surface by radio-frequency magnetron sputtering, followed by vacuum brazing of the AlN ceramic to an Al substrate using an Al–10.5Si–1.5 Mg(wt.%) filler metal. Brazing was conducted at 550–590 °C for 20 min to investigate the effects of brazing temperature on the joint microstructure, mechanical properties. During cooling, the preferential growth of α-Al rejected Si into the residual liquid, resulting in local Si enrichment within the brazing seam. Among the investigated conditions, the joint brazed at 580 °C exhibited the most uniform brazing seam and achieved the highest shear strength of 55 ± 2 MPa. The 580 °C joint exhibited an effective thermal conductivity of 196.3 W m−1 K−1 at 25 °C. These results demonstrate the feasibility of low-temperature AlN/Al joining using Al metallization and Al–Si–Mg filler metal, with potential applications in electronic thermal-management components.
KW - AlN/Al joints
KW - Al–Si–Mg filler metal
KW - Magnetron sputtering
KW - Thermal conductivity
KW - Vacuum brazing
UR - https://www.scopus.com/pages/publications/105052700504
U2 - 10.1016/j.ceramint.2026.10.077
DO - 10.1016/j.ceramint.2026.10.077
M3 - Article
AN - SCOPUS:105052700504
SN - 0272-8842
JO - Ceramics International
JF - Ceramics International
ER -