T1 - High-temperature interaction of nanostructured Lu2Si2O7 environmental barrier coatings with CMAS melts at 1400°C
AU - Guo, Donghui
AU - Jin, Runze
AU - Xu, Baosheng
N1 - Publisher Copyright:
© University of Science and Technology Beijing 2026.
PY - 2026/2
Y1 - 2026/2
N2 - The high-temperature interaction of nanostructured Lu2Si2O7 environmental barrier coatings (EBCs) with calcium–magnesium–aluminosilicate (CMAS) was investigated at 1400°C for 1, 10, 25, and 50 h to evaluate the coating’s resistance to CMAS corrosion. The results indicate a phase transformation over time, transitioning from Ca2Lu8(SiO4)6O2 apatite and Lu2Si2O7 to solely Lu2Si2O7. The interaction of the Lu2Si2O7 coating with the CMAS melts was divided into three stages based on the corrosion reaction behavior. The delamination cracks were distributed throughout the interface between the Si bond layer and Lu2Si2O7 layer after corroded at 1400°C for 50 h, signifying coating failure. In addition, the influence of monosilicates, disilicates, and corrosion duration on the recession layer thickness was analyzed by comparing previous reports on RE2SiO5/RE2Si2O7 coatings (RE = Gd, Yb, Lu, Er). Furthermore, the variation in the thermally grown oxide layer thickness in CMAS-corroded Lu2Si2O7 coatings was systematically investigated.
AB - The high-temperature interaction of nanostructured Lu2Si2O7 environmental barrier coatings (EBCs) with calcium–magnesium–aluminosilicate (CMAS) was investigated at 1400°C for 1, 10, 25, and 50 h to evaluate the coating’s resistance to CMAS corrosion. The results indicate a phase transformation over time, transitioning from Ca2Lu8(SiO4)6O2 apatite and Lu2Si2O7 to solely Lu2Si2O7. The interaction of the Lu2Si2O7 coating with the CMAS melts was divided into three stages based on the corrosion reaction behavior. The delamination cracks were distributed throughout the interface between the Si bond layer and Lu2Si2O7 layer after corroded at 1400°C for 50 h, signifying coating failure. In addition, the influence of monosilicates, disilicates, and corrosion duration on the recession layer thickness was analyzed by comparing previous reports on RE2SiO5/RE2Si2O7 coatings (RE = Gd, Yb, Lu, Er). Furthermore, the variation in the thermally grown oxide layer thickness in CMAS-corroded Lu2Si2O7 coatings was systematically investigated.
KW - calcium–magnesium–aluminosilicate
KW - corrosion
KW - environmental barrier coatings
KW - rare-earth disilicate
KW - thermal grown oxide
UR - https://www.scopus.com/pages/publications/105029162159
U2 - 10.1007/s12613-025-3126-6
DO - 10.1007/s12613-025-3126-6
M3 - Article
AN - SCOPUS:105029162159
SN - 1674-4799
VL - 33
SP - 737
EP - 748
JO - International Journal of Minerals, Metallurgy and Materials
JF - International Journal of Minerals, Metallurgy and Materials
IS - 2
ER -