TY - JOUR
T1 - Femtosecond laser-induced microgroove texturing of RMI/CVD-SiC dual transition layers for enhanced ablation resistance of ZrB2-SiC coatings
AU - Gao, Zhiting
AU - Ma, Zhuang
AU - Sun, Wanting
AU - Liu, Yanbo
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/11/1
Y1 - 2026/11/1
N2 - The rapid oxidation and ablation of C/C composites under high-temperature oxidizing environments severely limit their application in thermal protection systems for hypersonic vehicles. In this study, a dual-transition SiC architecture was fabricated by combining reaction melt infiltration (RMI) and chemical vapor deposition (CVD) to enhance the ablation resistance of ZrB2-SiC coatings through interface engineering. The influences of RMI/CVD SiC dual transition layers on the interfacial characteristics, microstructure evolution and ablation behavior were systematically investigated under the oxy-acetylene ablation at 2200-2600 °C for 600 s. Notably, the microgroove structure can produce the interlocking interface with the top coating, resulting in an interfacial bonding strength of 8.31 MPa. Under an extreme ablation condition of 2600 °C for 600 s, the RMI/CVD SiC dual transition layer system exhibits a low mass ablation rate of 1.1±0.12 × 10−4 g·s−1 while maintaining an intact coating structure, demonstrating significantly superior performance compared with the single-layered CVD-SiC and RMI-SiC systems. Based on microstructure observation and elemental distribution analysis, a temperature-dependent ablation mechanism was constructed, involving thermal shock, oxidation-volatilization coupling, crack propagation accompanied by SiO2 formation, and ultimate structural failure. The enhanced ablation resistance is primarily attributed to the synergistic effects of interfacial stress redistribution, crack suppression induced by the femtosecond laser-induced microgroove structure, oxygen diffusion inhibition, and oxidation-induced SiO2 sealing. This work can provide an effective interface-engineering strategy for the development of ultra-high-temperature ceramic coatings with excellent ablation resistance and durability under extreme aero-thermal environments.
AB - The rapid oxidation and ablation of C/C composites under high-temperature oxidizing environments severely limit their application in thermal protection systems for hypersonic vehicles. In this study, a dual-transition SiC architecture was fabricated by combining reaction melt infiltration (RMI) and chemical vapor deposition (CVD) to enhance the ablation resistance of ZrB2-SiC coatings through interface engineering. The influences of RMI/CVD SiC dual transition layers on the interfacial characteristics, microstructure evolution and ablation behavior were systematically investigated under the oxy-acetylene ablation at 2200-2600 °C for 600 s. Notably, the microgroove structure can produce the interlocking interface with the top coating, resulting in an interfacial bonding strength of 8.31 MPa. Under an extreme ablation condition of 2600 °C for 600 s, the RMI/CVD SiC dual transition layer system exhibits a low mass ablation rate of 1.1±0.12 × 10−4 g·s−1 while maintaining an intact coating structure, demonstrating significantly superior performance compared with the single-layered CVD-SiC and RMI-SiC systems. Based on microstructure observation and elemental distribution analysis, a temperature-dependent ablation mechanism was constructed, involving thermal shock, oxidation-volatilization coupling, crack propagation accompanied by SiO2 formation, and ultimate structural failure. The enhanced ablation resistance is primarily attributed to the synergistic effects of interfacial stress redistribution, crack suppression induced by the femtosecond laser-induced microgroove structure, oxygen diffusion inhibition, and oxidation-induced SiO2 sealing. This work can provide an effective interface-engineering strategy for the development of ultra-high-temperature ceramic coatings with excellent ablation resistance and durability under extreme aero-thermal environments.
KW - Ablation resistance
KW - Chemical vapor deposition (CVD)
KW - Dual transition layers
KW - Femtosecond laser texturing
KW - Reaction melt infiltration (RMI)
KW - Ultra-high temperature ceramics (UHTCs)
UR - https://www.scopus.com/pages/publications/105053333526
U2 - 10.1016/j.surfin.2026.110951
DO - 10.1016/j.surfin.2026.110951
M3 - Article
AN - SCOPUS:105053333526
SN - 2468-0230
VL - 100
JO - Surfaces and Interfaces
JF - Surfaces and Interfaces
M1 - 110951
ER -