摘要
Experiments have been performed to enhance negative thermal expansion (NTE) in the La(Fe,Co,Si)13-based compounds by optimizing the chemical composition, i.e., proper substitution of La by magnetic element Pr. It is found that increasing the absolute value of the average coefficient of thermal expansion (CTE) in the NTE temperature region (200-300 K) attributes to enhancement of the spontaneous magnetization and its growth rate with increasing Pr content. Typically, the average CTE of La1-xPrxFe 10.7Co0.8Si1.5 with x = 0.5 reaches as large as -38.5 × 10-6 K-1 between 200 and 300 K (δT = 100 K), which is 18.5% larger than that of x = 0. The present results highlight the potential applications of La(Fe,Co,Si)13-based compounds with a larger NTE coefficient.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 5869-5873 |
| 页数 | 5 |
| 期刊 | Inorganic Chemistry |
| 卷 | 53 |
| 期 | 11 |
| DOI | |
| 出版状态 | 已出版 - 2 6月 2014 |
| 已对外发布 | 是 |
学术指纹
探究 'Enhanced negative thermal expansion in La1- xPr xFe10.7Co0.8Si1.5 compounds by doping the magnetic rare-earth element praseodymium' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver