摘要
The pre-soaking procedure was developed to identify the grain refining effects on Al2O3 ceramic during spark plasma sintering (SPS). The results showed the micrometer-size Al2O3 single crystal particles refined by the thermo-electric-mechanical mechanism. The large sized single crystal particles have more obvious grain refining and show more refined spots. A time dependent grain refining process has been identified after the powders were soaked longer at temperatures below the grain growth levels. Our work demonstrates a possible method to make nanostructured ceramic using SPS with pre-soaking process.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 13414-13418 |
| 页数 | 5 |
| 期刊 | Ceramics International |
| 卷 | 44 |
| 期 | 11 |
| DOI | |
| 出版状态 | 已出版 - 1 8月 2018 |
| 已对外发布 | 是 |