TY - JOUR
T1 - Effect of decarburization temperature on the microstructure, texture, and magnetic property of industrial low-temperature grain-oriented silicon steel
AU - Xu, Ning
AU - Jia, Zhiwei
AU - Zhang, Haili
AU - Liu, Xuming
AU - Gao, Hongwei
AU - Xuan, Dongpo
AU - Wang, Junsheng
N1 - Publisher Copyright:
Copyright © 2026. Published by Elsevier B.V.
PY - 2026/12
Y1 - 2026/12
N2 - This study systematically investigates the impact of decarburization temperature on the microstructure, texture, and magnetic properties of a 0.23 mm-thick industrial low-temperature grain-oriented (LTGO) silicon steel. It is demonstrated that the decarburization temperature significantly influences the sharpness of Goss texture ({110}〈001〉) and the resultant magnetic performance by modulating the primary recrystallized grain size, texture components, and grain boundary character distribution. At 845 °C, a moderate primary grain size was obtained, coupled with increased volume fractions of {114}〈481〉 and {111}〈112〉 textures, which effectively facilitate the abnormal growth of Goss grains. Furthermore, the highest proportion of Σ9 boundaries and the lowest fraction of Σ3 boundaries were observed, consistent with the high-energy boundary theory, thereby promoting selective growth of Goss grains. Consequently, complete secondary recrystallization with a sharp Goss texture and optimal magnetic properties (P17/50 = 0.92 W/kg, B8 = 1.89 T) was achieved. Any deviation from this temperature led to a deterioration in secondary recrystallization and magnetic performance. This work provides both theoretical and experimental insights for optimizing the magnetic properties of industrial LTGO silicon steel.
AB - This study systematically investigates the impact of decarburization temperature on the microstructure, texture, and magnetic properties of a 0.23 mm-thick industrial low-temperature grain-oriented (LTGO) silicon steel. It is demonstrated that the decarburization temperature significantly influences the sharpness of Goss texture ({110}〈001〉) and the resultant magnetic performance by modulating the primary recrystallized grain size, texture components, and grain boundary character distribution. At 845 °C, a moderate primary grain size was obtained, coupled with increased volume fractions of {114}〈481〉 and {111}〈112〉 textures, which effectively facilitate the abnormal growth of Goss grains. Furthermore, the highest proportion of Σ9 boundaries and the lowest fraction of Σ3 boundaries were observed, consistent with the high-energy boundary theory, thereby promoting selective growth of Goss grains. Consequently, complete secondary recrystallization with a sharp Goss texture and optimal magnetic properties (P17/50 = 0.92 W/kg, B8 = 1.89 T) was achieved. Any deviation from this temperature led to a deterioration in secondary recrystallization and magnetic performance. This work provides both theoretical and experimental insights for optimizing the magnetic properties of industrial LTGO silicon steel.
KW - Low-temperature grain-oriented silicon steel
KW - Magnetic properties
KW - Microstructure
KW - Texture
UR - https://www.scopus.com/pages/publications/105051469062
U2 - 10.1016/j.mlblux.2026.100286
DO - 10.1016/j.mlblux.2026.100286
M3 - Article
AN - SCOPUS:105051469062
SN - 2590-1508
VL - 28
JO - Materials Letters: X
JF - Materials Letters: X
M1 - 100286
ER -