N2 - This work investigates the dynamic fracture of Al and Sn rods using thermomechanically coupled mechanical simulation, with emphasis on the roles of tensile speed, temperature and geometry. Both Al and Sn exhibit a systematic sequence of fracture-mode transitions as the tensile speed increases. When the tensile speed v is low, the entire rod can be approximately regarded as having the same strain rate (ε˙=2v/L), fracture initiation is highly sensitive to small perturbations and appears spatially stochastic. At intermediate tensile speed, the interaction of tensile stress waves becomes the dominant mechanism, leading to fracture in the central region of the rod or on both its sides. Once the tensile speed exceeds a critical threshold, fracture shifts toward the loaded ends because of the inertia-constrained localization near the loading boundaries. Initial temperature will enhance thermal softening, especially for Sn, which has a relatively low melting point. Furthermore, the fracture strength follows a power-law relationship with the aspect ratio: increasing aspect ratio enhances the apparent fracture strength by reducing radial dispersion and promoting more one-dimensional tensile-wave transmission. Based on the finite-element data within the solid-state validity range, a structural empirical relation incorporating tensile speed, initial temperature, and aspect ratio is proposed to correlate the nominal dynamic tensile fracture strength. This relation describes an apparent structural response of the rod rather than an intrinsic material constitutive law.
AB - This work investigates the dynamic fracture of Al and Sn rods using thermomechanically coupled mechanical simulation, with emphasis on the roles of tensile speed, temperature and geometry. Both Al and Sn exhibit a systematic sequence of fracture-mode transitions as the tensile speed increases. When the tensile speed v is low, the entire rod can be approximately regarded as having the same strain rate (ε˙=2v/L), fracture initiation is highly sensitive to small perturbations and appears spatially stochastic. At intermediate tensile speed, the interaction of tensile stress waves becomes the dominant mechanism, leading to fracture in the central region of the rod or on both its sides. Once the tensile speed exceeds a critical threshold, fracture shifts toward the loaded ends because of the inertia-constrained localization near the loading boundaries. Initial temperature will enhance thermal softening, especially for Sn, which has a relatively low melting point. Furthermore, the fracture strength follows a power-law relationship with the aspect ratio: increasing aspect ratio enhances the apparent fracture strength by reducing radial dispersion and promoting more one-dimensional tensile-wave transmission. Based on the finite-element data within the solid-state validity range, a structural empirical relation incorporating tensile speed, initial temperature, and aspect ratio is proposed to correlate the nominal dynamic tensile fracture strength. This relation describes an apparent structural response of the rod rather than an intrinsic material constitutive law.
KW - Aspect ratio
KW - Dynamic fracture
KW - Initial temperature
KW - Tensile speed
KW - Thermomechanical coupling
UR - https://www.scopus.com/pages/publications/105048682602
U2 - 10.1016/j.euromechsol.2026.106339
DO - 10.1016/j.euromechsol.2026.106339
M3 - Article
AN - SCOPUS:105048682602
SN - 0997-7538
VL - 121
JO - European Journal of Mechanics, A/Solids
JF - European Journal of Mechanics, A/Solids
M1 - 106339
ER -