摘要
Hydrogen internal combustion engines offer zero carbon emissions and high power output, but widespread adoption is hindered by the rapid wear failure of direct injector valves in unlubricated hydrogen environments. This study systematically investigates the dynamic impact wear and oxidation mechanisms of high-strength sealing steels. Explicit finite element simulations and cyclic impact tests establish a baseline, revealing a transition from initial plastic cratering to steady-state surface wear. Comparative experiments on uncharged and pre-charged specimens decouple the environmental influence, uncovering a coupled mechanochemical competition triggered by hydrogen. Chemically, the hydrogen-rich atmosphere mitigates third-body abrasive wear by suppressing interfacial oxidation through the tribochemical reduction of nascent oxides. Mechanically, however, hydrogen ingress induces matrix embrittlement and toughness degradation, overriding the chemical benefit and driving extensive shallow brittle spallation that exacerbates total wear volume. Decoupling these competing mechanisms provides essential theoretical guidance for developing durable dynamic sealing pairs in hydrogen systems.
| 源语言 | 英语 |
|---|---|
| 期刊论文编号 | 111587 |
| 期刊 | Engineering Failure Analysis |
| 卷 | 199 |
| DOI | |
| 出版状态 | 已出版 - 1 1月 2027 |
| 已对外发布 | 是 |
学术指纹
探究 'Dynamic impact wear and hydrogen-assisted failure mechanisms of sealing steels for high-pressure hydrogen injectors' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver