N2 - Aviation flared pipe fittings are subjected to complex multidirectional vibration, which induces nonuniform contact redistribution and localized sealing degradation. This study develops a history-dependent, direction-resolved cross-scale framework coupling elastoplastic finite-element analysis, CG-FFT rough-surface contact calculation, and three-dimensional leakage simulation, together with experiments under three prescribed vibration modes. Cyclic local contact states at representative circumferential directions are transferred to the microscopic model to capture leakage evolution beyond conventional averaged quantities. Results show that leakage is governed by directional low-pressure pathways rather than by mean contact pressure or a universally most detrimental vibration mode. Extended 40-cycle calculations further reveal history-dependent leakage-path reconfiguration under different vibration amplitudes, with the 0.4 mm case exhibiting the strongest late-cycle variability. Parametric analyses of preload, surface roughness, oil-temperature-dependent viscosity, and excitation frequency further characterize the sealing response. Although leakage decreases continuously with increasing preload under static conditions, a pronounced rebound occurs at high preload under rotational-bending and coupled vibration. Increasing the areal RMS roughness from 0.8 to 1.6 μm amplifies the mean leakage by approximately 29–36 times and makes vibration-mode differences secondary. Under a fixed 0.3 mm displacement envelope, the 5–500 Hz sensitivity analysis reveals an increasingly inertia-sensitive macroscopic structural response, while the roughness-scale flow remains quasi-steady. Experiments under the three vibration modes reveal torque-dependent crossovers in the mean leakage responses, providing trend-level evidence that sealing degradation depends jointly on vibration path and tightening condition.
AB - Aviation flared pipe fittings are subjected to complex multidirectional vibration, which induces nonuniform contact redistribution and localized sealing degradation. This study develops a history-dependent, direction-resolved cross-scale framework coupling elastoplastic finite-element analysis, CG-FFT rough-surface contact calculation, and three-dimensional leakage simulation, together with experiments under three prescribed vibration modes. Cyclic local contact states at representative circumferential directions are transferred to the microscopic model to capture leakage evolution beyond conventional averaged quantities. Results show that leakage is governed by directional low-pressure pathways rather than by mean contact pressure or a universally most detrimental vibration mode. Extended 40-cycle calculations further reveal history-dependent leakage-path reconfiguration under different vibration amplitudes, with the 0.4 mm case exhibiting the strongest late-cycle variability. Parametric analyses of preload, surface roughness, oil-temperature-dependent viscosity, and excitation frequency further characterize the sealing response. Although leakage decreases continuously with increasing preload under static conditions, a pronounced rebound occurs at high preload under rotational-bending and coupled vibration. Increasing the areal RMS roughness from 0.8 to 1.6 μm amplifies the mean leakage by approximately 29–36 times and makes vibration-mode differences secondary. Under a fixed 0.3 mm displacement envelope, the 5–500 Hz sensitivity analysis reveals an increasingly inertia-sensitive macroscopic structural response, while the roughness-scale flow remains quasi-steady. Experiments under the three vibration modes reveal torque-dependent crossovers in the mean leakage responses, providing trend-level evidence that sealing degradation depends jointly on vibration path and tightening condition.
KW - Complex vibration conditions
KW - Coupled vibration
KW - Cross-scale analysis
KW - Leakage rate
KW - Sealing performance
UR - https://www.scopus.com/pages/publications/105052475121
U2 - 10.1016/j.engfailanal.2026.111536
DO - 10.1016/j.engfailanal.2026.111536
M3 - Article
AN - SCOPUS:105052475121
SN - 1350-6307
VL - 198
JO - Engineering Failure Analysis
JF - Engineering Failure Analysis
M1 - 111536
ER -