跳到主要导航 跳到搜索 跳到主要内容

Catalytic activity for methane combustion of the perovskite-type La1-xSrxCoO3-δ oxide prepared by the urea decomposition method

  • Zhiming Gao*
  • , Ruiyan Wang
  • *此作品的通讯作者
  • Ministry of Education in China

科研成果: 期刊稿件 › 文章 › 同行评审

摘要

Four methods were adopted to prepare perovskite-type oxide with molar ratio of La/Sr/Co = 0.9/0.1/1.0. The oxide prepared by the urea decomposition method showed the highest catalytic activity for methane combustion and a good durability at 600 °C for 90. h. Surface structure features of this oxide were discussed by use of XPS data. This method was further applied to prepare other perovskite oxides with nominal degree of substitution x= 0.0, 0.2 and 0.3. Relation of catalytic activity with degree of substitution was discussed in view of cooperation of surface lattice oxygen vacancy with surrounding cobalt ions at lower oxidation states.

源语言英语
页(从-至)147-153
页数7
期刊Applied Catalysis B: Environmental
卷98
期3-4
DOI
出版状态已出版 - 8月 2010
已对外发布是

学术指纹

探究 'Catalytic activity for methane combustion of the perovskite-type La1-xSrxCoO3-δ oxide prepared by the urea decomposition method' 的科研主题。它们共同构成独一无二的学术指纹。

引用此