摘要
This study investigates the mechanical properties and failure mechanisms of tungsten heavy alloys (WHAs) fabricated via binder jetting (BJT)—an indirect additive manufacturing technique—versus conventional liquid-phase sintering (LPS) across wide strain-rate regimes. A 93W-5Ni-2Fe alloy printed by BJT with subsequent heat treatment exhibits a microstructure of W particles within a Ni-Fe binder phase. BJT-processed WHAs demonstrate approximately doubled W particle size and marginally higher W-W contiguity (CW-W≈0.307) than LPS counterparts (CW-W≈0.291). Quasi-static tensile tests reveal 17.3 % and 4.8 % higher yield and tensile strength for BJT WHAs relative to LPS, yet reduced elongation (24.5 % vs. 39.0 %). The dominant fracture mode transitions from ductile (LPS) to mixed brittle-ductile in BJT, characterized by tungsten cleavage (“river patterns”) and binder-phase dimples. Dynamic compression (1000–5000 s−1) indicates lower compressive strength and strain-rate sensitivity in BJT WHAs. Ballistic evaluations confirm comparable penetration performance (within 3 %) between BJT and LPS long-rod penetrators under extreme conditions. Residual penetrator analysis identifies penetration failure mechanisms: mushroom-head segmentation via structural-design-induced macrocracks and adiabatic shear band (ASB)-derived microcracks. This work establishes a foundation for BJT WHAs in the field of impact dynamics.
| 源语言 | 英语 |
|---|---|
| 文章编号 | 149192 |
| 期刊 | Materials Science and Engineering: A |
| 卷 | 947 |
| DOI | |
| 出版状态 | 已出版 - 12月 2025 |
| 已对外发布 | 是 |
指纹
探究 'An investigation of static, dynamic, and extreme dynamic strain rate properties in binder jetting tungsten heavy alloys' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver