TY - JOUR
T1 - A rigid-flexible approach enables high-performance elastomers with broad damping temperature range and enhanced strength for vibration attenuation and impact resistance
AU - Shang, Jialu
AU - Li, Xiaodong
AU - Sun, Shuping
AU - Yang, Lei
AU - Zhang, Xinbei
AU - Sun, Yue
AU - Xu, Chang
AU - Zhu, Youqi
AU - Zhang, Xufeng
AU - Jiang, Hao
AU - Zou, Meishuai
N1 - Publisher Copyright:
© 2026
PY - 2026/12/1
Y1 - 2026/12/1
N2 - Designing elastomers that combine high mechanical strength with a broad damping-temperature range remains a major challenge for vibration attenuation and impact protection. Here, flexible 2, 4-pentanedione dioxime (2,4-PD) and rigid 2, 6-diaminopyridine (2,6-DAP) were used as complementary chain extenders to regulate the aggregation structure of poly(oxime-urethane-urea) (POUU) elastomers. The optimized POUU-P0.4D0.6 features local short-range order and long-range weak microphase separation. This hierarchical structure affords a tensile strength of 52.33 MPa, an elongation at break of 920.20%, and an effective damping-temperature range of 122.84 ℃ (12.9–135.7 ℃, tan δ ≥ 0.3). Temperature-dependent structural and spectroscopic results, together with calculated interaction energies, associate the broad damping response with sequential soft-segment relaxation, interfacial friction, and reorganization of locally associated domains. Repeated temperature scans, rate-dependent cyclic tensile tests, falling-ball measurements, and high-strain-rate compression further characterize the energy-dissipation and impact responses. These results establish a rigid-flexible molecular strategy for high-strength damping elastomers operating from room temperature to elevated temperatures.
AB - Designing elastomers that combine high mechanical strength with a broad damping-temperature range remains a major challenge for vibration attenuation and impact protection. Here, flexible 2, 4-pentanedione dioxime (2,4-PD) and rigid 2, 6-diaminopyridine (2,6-DAP) were used as complementary chain extenders to regulate the aggregation structure of poly(oxime-urethane-urea) (POUU) elastomers. The optimized POUU-P0.4D0.6 features local short-range order and long-range weak microphase separation. This hierarchical structure affords a tensile strength of 52.33 MPa, an elongation at break of 920.20%, and an effective damping-temperature range of 122.84 ℃ (12.9–135.7 ℃, tan δ ≥ 0.3). Temperature-dependent structural and spectroscopic results, together with calculated interaction energies, associate the broad damping response with sequential soft-segment relaxation, interfacial friction, and reorganization of locally associated domains. Repeated temperature scans, rate-dependent cyclic tensile tests, falling-ball measurements, and high-strain-rate compression further characterize the energy-dissipation and impact responses. These results establish a rigid-flexible molecular strategy for high-strength damping elastomers operating from room temperature to elevated temperatures.
KW - Broad damping-temperature range
KW - High strength
KW - Impact resistance
KW - POUU elastomer
KW - Rigid-flexible strategy
KW - Vibration attenuation
UR - https://www.scopus.com/pages/publications/105053338467
U2 - 10.1016/j.cej.2026.182900
DO - 10.1016/j.cej.2026.182900
M3 - Article
AN - SCOPUS:105053338467
SN - 1385-8947
VL - 549
JO - Chemical Engineering Journal
JF - Chemical Engineering Journal
M1 - 182900
ER -