Skip to main navigation Skip to search Skip to main content

Valorization of hazardous phosphating sludge: construction of a carbon-rich, heterointerfacial, halogen-free and all-in-one flame retardant for silicone rubber

  • Ziyang Zhang
  • , Wen Wang
  • , Xiaoyang Guo
  • , Jing He
  • , Junwen Xu
  • , Zaihang Zheng
  • , Ye Tang Pan*
  • *Corresponding author for this work
  • Changchun University of Technology
  • Beijing Institute of Technology

Research output: Contribution to journal › Article › peer-review

Abstract

Silicone rubber (SR) was widely used in fire-sensitive applications, but its inherent flammability remained a major limitation. Conventional flame-retardant modification often relied on a high loading of inorganic additives or multi-component intumescent system, which might cause poor interfacial compatibility, high filler demand, and deterioration of mechanical strength. Meanwhile, hazardous phosphating sludge generated from automotive pretreatment process was a disposal-restricted industrial by-product rich in inorganic phosphates and metal oxide phases, making it a potentially useful inorganic component for flame-retardant structural design and waste valorization. In this work, a single-component integrated flame retardant (Si-WR@MS@DTMA) was prepared through a multistage assembly strategy. Phosphating waste residue (WR) was used as an inorganic skeleton, a hydroxyethyl-cellulose-derived carbonaceous interlayer was constructed on its surface, a melamine/diethylenetriamine penta(methylene phosphonic acid)-derived phosphorus‑nitrogen layer was subsequently deposited, and epoxy-modified silicone resin (EPSR) was introduced for interfacial regulation. With 25 phr Si-WR@MS@DTMA, the resulting SR composite exhibited a LOI of 29.5%, achieved a UL-94 V-0 rating, a pHRR reduction of 42.9% and a THR reduction of 17.2%, respectively. Its glow-wire ignition temperature (GWIT) was increased to 875 ± 25 °C, and the mass loss after 5 min flame impingement test was only 8.0%. The enhanced flame retardancy was associated with inorganic skeletal support, enhanced retention of carbonaceous structures, phosphorus/nitrogen-assisted residue construction, and the suppressed release of combustible cyclic siloxane products. In addition, the Young's modulus was increased by 500%, while the elongation at break remained at 207%. This work provided a feasible strategy for the value-added utilization of industrial solid waste and the design of mechanically reliable flame-retarding SR composites.

Original languageEnglish
Article numbere02278
JournalSustainable Materials and Technologies
Volume50
DOIs
Publication statusPublished - 15 Dec 2026
Externally publishedYes

Keywords

  • Ablation resistance
  • Phosphate-rich inorganic waste residue
  • Silicone rubber
  • Single-component flame retardant

Fingerprint

Dive into the research topics of 'Valorization of hazardous phosphating sludge: construction of a carbon-rich, heterointerfacial, halogen-free and all-in-one flame retardant for silicone rubber'. Together they form a unique fingerprint.

Cite this