Thermal runaway behavior and features of LiFePO4/graphite aged batteries under overcharge

  • Cong jie Wang
  • , Yan li Zhu*
  • , Fei Gao
  • , Chuang Qi
  • , Peng long Zhao
  • , Qing fen Meng
  • , Jian yong Wang
  • , Qi bing Wu
  • *Corresponding author for this work
  • Beijing Institute of Technology
  • State Grid Corporation of China
  • Ltd.
  • Qaidam Xinghua Lithium Salt Co. Ltd.
  • Guizhou Meiling Power Sources Co. Ltd

Research output: Contribution to journalArticlepeer-review

Abstract

In this paper, the overcharge tests of 25 Ah LiFePO4/graphite batteries are conducted in an open environment and the overcharge-to-thermal-runaway characteristics are studied. The effects of current rates (C-rates: 2C, 1C, 0.5C, and 0.3C) and states of health (SOHs: 100%, 80%, 70%, and 60%) on thermal runaway features are discussed in detail. The overcharge process can be summarized into five stages based on the experimental phenomena (C-rate ≥ 1 and SOH ≥ 80%): expansion, fast venting after safety valve rupture, slow venting, intense jet smoke, and explosion, while the battery cannot explode at lower C-rates and SOHs. The maximum pressure increases with the increase in C-rate or SOH. There are five obvious inflection points in the voltage curve during overcharge process. The V1 (point B) of aged battery, corresponding to lithium plating on the anode, changes little with C-rates. It is slightly lower than that of the new battery. A sharp drop in voltage (point E) is probably due to the internal short circuit (ISC), caused by the local melting and rupture of the separator. It takes more than 2 minutes from the moment of ISC to thermal runaway regardless of the SOH, indicating that there are a few minutes to take safety measures if the voltage is an indication parameter. The onset temperature of thermal runaway decreases first and then increases as the SOH decreases from 100% to 60% during 1C constant overcharge tests. These results can provide guidance for the thermal management of the whole battery life cycle and the reuse of retired batteries.

Original languageEnglish
Pages (from-to)5477-5487
Number of pages11
JournalInternational Journal of Energy Research
Volume44
Issue number7
DOIs
Publication statusPublished - 10 Jun 2020

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

Keywords

  • SOH
  • ageing
  • lithium-ion battery safety
  • overcharge
  • thermal runaway

Fingerprint

Dive into the research topics of 'Thermal runaway behavior and features of LiFePO4/graphite aged batteries under overcharge'. Together they form a unique fingerprint.

Cite this