Skip to main navigation Skip to search Skip to main content

Regulation of layered grain heterostructure in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing

  • Beijing Institute of Technology
  • Tangshan Research Institute

Research output: Contribution to journal › Conference article › peer-review

Abstract

Heterostructure is a novel microstructure to break the strength and ductility trade-off of materials. In this study, the layered grain heterostructure with tailored grain size and layer thickness was successfully fabricated in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing via alternately modulating the laser process parameters in the adjacent layers. The average grain sizes in the fine and coarse grain layers were ~20 μm and ~53 μm, respectively, and their corresponding layer thicknesses were ~320 μm and ~280 μm under volumetric energy density (VED) of 222 and 167 J/mm3 and scanning speeds of 20 and 15 mm/s, respectively. When the VED was increased to 300 J/mm3, and the scanning speed was lowered to 10 mm/s, the grain size in the fine grain layer could be refined to ~10 μm, and the ratio of the fine and coarse grain sizes reached 1/5, which is expected to induce pronounced hetero-deformation-induced (HDI) strengthening. The grain size refinement is ascribed to the increasing cooling rate at the melt pool boundary at higher VED and lower scanning speed, as suggested by the simulation. The research findings in this paper provide valuable references for the regulation of heterostructures.

Original languageEnglish
Article number022051
JournalJournal of Physics: Conference Series
Volume3254
Issue number2
DOIs
Publication statusPublished - 2026
Externally publishedYes
Event2026 9th International Conference on Mechanical, Electrical and Material Application, MEMA 2026 - , China
Duration: 27 Mar 2026 → 29 Mar 2026

Fingerprint

Dive into the research topics of 'Regulation of layered grain heterostructure in Ti-Zr-V-Nb-Al-Mo lightweight high-entropy alloy by laser additive manufacturing'. Together they form a unique fingerprint.

Cite this