Morphology controlling technique for submicron CL-20

Li Yang*, Shao Zong Wang, Peng Juan Zhao, Tong Lai Zhang

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

12 Citations (Scopus)

Abstract

The submicron CL-20 was prepared by solvent-nonsolvent method with different surfactants, and the influence factors about various kinds, quality and injecting styles of surfactants were analyzed. Results show that the uniform and block-like CL-20 with 1 μm, 2 μm are obtained using 2 g raw materials CL-20 with 3.5 mL 2% polyvinyl alcohol (PV), and with 6.5 mL 5% polyoxyethylene ether (PT) respectively. The particle with 1 μm and elliptoid uniform and narrow particle-size distribution are obtained by watering pot injecting method with 6.5 mL 5% PT. CL-20 has higher heat sensitivity and is still ε polymorph after fine.

Original languageEnglish
Pages (from-to)254-257
Number of pages4
JournalHanneng Cailiao/Chinese Journal of Energetic Materials
Volume16
Issue number3
Publication statusPublished - Jun 2008

Keywords

  • CL-20
  • Materials science
  • Solvent-nonsolvent method
  • Submicron
  • Surfactant

Fingerprint

Dive into the research topics of 'Morphology controlling technique for submicron CL-20'. Together they form a unique fingerprint.

Cite this